Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Voloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Ultimate 108 MPa
15700 psi
ASTM D638
Elongation at Break 3.7 %
3.7 %
ASTM D638
Flexural Strength 157 MPa
22800 psi
ASTM D790
Flexural Modulus 9.50 GPa
1380 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.96 J/cm
9.29 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 258 - 268 °C
496 - 514 °F
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 296 - 304 °C
565 - 579 °F