Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.74 g/cc | 0.0629 lb/in³ | Laminate |
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT PX11311U PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6 compliant with ECO protocols, non-brominated, non chlorinated |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50004 Anti-blocking Masterbatch LDPE. 70% CaCO3 FilledInformation provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 50004 Anti-split HPP. 70% CaCO3 Filled.Thermal Resistance.Information provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP 2C004 ETFE LNP* THERMOCOMP* 2C004 is a compound based on ETFE resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Toho Tenax Besfight® G40-600 12K IMA-7C EP03 Continuous Filament Carbon Fiber Intermediate Modulus; Collimated; Polyacrylonitrile (PAN) based fiberTypical values; measured by Toho Strand Test Method based on JIS R7601 for fiber selection purposes. Information provided by Toho.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive) Carbon-powder-filled, thermally stable, conductive material with consistent resistivities |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-78 Compression Molded PPS Compound, 47% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Dry) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Applied Composites 175 Vinylester SMC Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | dry; ISO 1183 |
BASF Ultramid® HMG13 HS BK-102 63% Glass Filled PA6 (Conditioned) Ultramid HMG13 HS BK-102 is a 63% glass filled, injection molding, high modulus nylon designed to have high strength and stiffness for metal replacement applications. It also has excellent moldabil.. |