UCAR Carbon UCAR® CS Extruded Graphite

Category Carbon , Graphite
Manufacturer UCAR Carbon Company (GrafTech International)
Trade Name UCAR®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UCAR Carbon UCAR® CS Extruded Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Densified prior to graphitization, Grade CS is an extruded graphite 25-30% higher in strength than CBY. Grade CS is a low ash graphite with an oxidation resistance similar to grade CBY. It is the material of choice for applications requiring higher densities, better mechanical strength, or less porosity than grade CBY. Grade CS is the most popular multi-purpose grade.In sizes less than 3” dia CS particle size is reduced to improve characteristics.Typical Applications:Casting molds and furnace parts for hot metalPowder metallurgyBoats and trays for sintering applicationsResistance heatingCrucibles for melting and alloyingFurnace componentsRefractory Systems applications such as blast furnace and submerged arc furnace liningsTabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
Particle Size <= 750 µm
<= 750 µm
Ash 0.090 %
0.090 %
Mechanical Properties Metric English Comments
Flexural Strength 22.1 MPa
3200 psi
Thermal Properties Metric English Comments
CTE, linear 2.50 µm/m-°C

@Temperature 20.0 - 100 °C
1.39 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 160 W/m-K
1110 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000750 ohm-cm
0.000750 ohm-cm