Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® B 218L V20 Black 44 N PA66, 25% glass fiber, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Copolyamide 66/6, reinforced with 20% of glass fiber, for injection molding, heat stabilized with improved UV ageing resistanceAvailable in: Asia Pacific and EuropeProduct Applications: TECHNYL B 218L V20 noir 44 N is used in all sectors of industry, offering an excellent combination of thermal and mechanical properties. This grade is commonly used for automotive applications which require a good surface appearance and a good UV resistance, such as: - external mirror housings and door handles. This product is available in black color.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ISO 527 Type 1A
Elongation at Break 9.0 %
9.0 %
ISO 527 Type 1A
Tensile Modulus 4.50 GPa
653 ksi
ISO 527 Type 1A
Flexural Modulus 3.50 GPa
508 ksi
ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
ISO 180/1eA
Charpy Impact Unnotched 8.30 J/cm²
39.5 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
ISO 179/1eA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
IEC 60093
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
IEC 60093
Dielectric Constant 4.0
4.0
IEC 60250
Dielectric Strength 28.0 kV/mm
711 kV/in
IEC 60243
Dissipation Factor 0.11
0.11
IEC 60250
Processing Properties Metric English Comments
Moisture Content <= 0.20 %
<= 0.20 %
Users viewing this material also viewed the following: