Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DL003 is a compound based on Polycarbonate resin containing PTFE.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
50 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa
7830 psi
50 mm/min; ISO 527
Elongation at Break 9.6 %
9.6 %
50 mm/min; ISO 527
Elongation at Yield 5.5 %
5.5 %
50 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Strength 84.0 MPa
12200 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) >= 100 kJ/m²
>= 47.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 74.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
41.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
41.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 128 °C
262 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af