Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-Brominated & Non-Chlorinated Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527
Tensile Strength, Yield 57.0 MPa
8270 psi
ISO 527
Elongation at Break 4.0 - 8.0 %
4.0 - 8.0 %
ISO 527
Elongation at Yield 3.8 %
3.8 %
ISO 527
Tensile Modulus 2.80 GPa
406 ksi
1 mm/min; ISO 527
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Izod Impact, Notched 1.22 J/cm

@Temperature 23.0 °C
2.29 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 17.88 J/cm

@Temperature 23.0 °C
33.50 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 11.0 kJ/m²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 85.0 kJ/m²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-1

@Thickness 1.60 mm
V-1

@Thickness 0.0630 in
UL 94
V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
UL 94
V-0

@Thickness 2.10 mm
V-0

@Thickness 0.0827 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D 257
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method
Copyright © lookpolymers.com All Rights Reserved