| Category | Polymer , Thermoplastic , Nylon , Nylon 46 , Nylon 46, Glass Fiber Reinforced |
| Manufacturer | DSM Engineering Plastics |
| Trade Name | Stanyl® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DSM Stanyl® TW200F3 (DAM) Nylon 46 15% Glass Reinforced, Heat Stabilized (North America).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
| Moisture Absorption at Equilibrium | 3.1 % | 3.1 % | 50% RH / 23°C; Similar to ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 140 MPa | 20300 psi | ISO 527-1/-2 |
| Elongation at Break | 4.0 % | 4.0 % | ISO 527-1/-2 |
| Tensile Modulus | 6.10 GPa | 885 ksi | ISO 527-1/-2 |
| Charpy Impact, Notched | 0.450 J/cm² | 2.14 ft-lb/in² | ISO 179/1eU |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 30.0 µm/m-°C @Temperature 20.0 °C |
16.7 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 90.0 µm/m-°C @Temperature 20.0 °C |
50.0 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
| Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
| Deflection Temperature at 1.8 MPa (264 psi) | 275 °C | 527 °F | ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Comparative Tracking Index | 400 V | 400 V | IEC 60112 |