Physical Properties Metric English Comments
Density 1.18 - 1.33 g/cc
0.0426 - 0.0480 lb/in³
Average value: 1.27 g/cc Grade Count:20
Overview of materials for PETG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.04 - 1.33 g/cc
0.0376 - 0.0480 lb/in³
Average value: 1.18 g/cc Grade Count:142
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Density 1.24 - 1.33 g/cc

@Temperature 270 - 290 °C
0.0448 - 0.0480 lb/in³

@Temperature 518 - 554 °F
Average value: 1.29 g/cc Grade Count:2
Overview of materials for Nylon 6, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E..
Density 1.11 - 1.33 g/cc
0.0401 - 0.0480 lb/in³
Average value: 1.19 g/cc Grade Count:7
Overview of materials for Nylon 66 Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66 Fiber". Each property range of values reported is minimum and maximum values of appropriate Mat..
Density 1.22 - 1.33 g/cc
0.0441 - 0.0480 lb/in³
Sibur O-40 Compound 239 Polyvinyl Chloride (PVC)
Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p..
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K002 PBT, Low Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K008 PBT, High Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K002 PBT, Low Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K006 PBT, Medium Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K008 PBT, High Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ASTM D792
Shinkong Synthetic Fibers Shinite® D201K011 PBT, Super Viscosity
Information from Shinkong Synthetic Fibers Corp.
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds CL 8315 Flexible PVC, Sheathing
Sheath coaxial TV Cable
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds GS 6530 Flexible PVC, Injection Molding for Footwear
Soles
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds GS 9015 Flexible PVC, Injection Molding for Footwear
Technical items for soles
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1184
Fainplast Compounds KL 94 Flexible PVC, Insulation for High Temperatures Lead Free
Automotive cables low thickness
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1184
Fainplast Compounds KL 95 Flexible PVC, Insulation for High Temperatures Lead Free
Automotive cables low thickness
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding
Anti impact connectors
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds MRT 256/G Medical Rigid PVC, Injection Molding
Beta and gamma resistant connectors
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds PM 5740 Flexible PVC, Extrusion
Gaskets for frames
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1184
Fainplast Compounds KL 95/3 Flexible PVC, Insulation for High Temperatures Lead Free
Operating temperature 90°C
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds PM 5840 Flexible PVC, Extrusion
Gaskets for frames
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Fainplast Compounds PM 8220 Flexible PVC, Lead Free
Various profiles
Density 1.24 - 1.33 g/cc
0.0448 - 0.0480 lb/in³
Average value: 1.29 g/cc Grade Count:24
Overview of materials for Polyphenylene Ether, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu..
Density 1.30 - 1.33 g/cc
0.0470 - 0.0480 lb/in³
RP-17617
Solvay RHODOLINE® 270 Surfactant
Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.Identification: ACRYLIC POLYMERCAS: 9003-04-7Available in: North America IR..