SABIC Innovative Plastics LNP FARADEX DS0036I PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX DS0036I PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-Brominated & Non-Chlorinated Flame Retardant.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0070 cm/cm

@Time 86400 sec
0.0040 - 0.0070 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 55.0 MPa
7980 psi
ISO 527
Tensile Strength, Yield 57.0 MPa
8270 psi
ISO 527
Elongation at Break 4.0 - 8.0 %
4.0 - 8.0 %
ISO 527
Elongation at Yield 3.8 %
3.8 %
ISO 527
Tensile Modulus 2.80 GPa
406 ksi
1 mm/min; ISO 527
Flexural Strength 80.0 MPa
11600 psi
ISO 178
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
Izod Impact, Notched 1.22 J/cm
2.29 ft-lb/in
ASTM D256
Izod Impact, Unnotched 17.88 J/cm
33.50 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 85.0 kJ/m²
40.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
37.2 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 56.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
31.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 136 °C
277 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 2.10 mm
V-0

@Thickness 0.0827 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257
Surface Resistance 100 - 1000 ohm
100 - 1000 ohm
ASTM D257
Shielding Effectiveness 40 - 55 dB

@Thickness 3.00 mm
40 - 55 dB

@Thickness 0.118 in
SABIC Method