Inno-Comp Ltd
Trade Name INNOPOL® CS
Trade Name :
INNOPOL® CS
Product List
Category
Polypropylene with 40% Talc Filler
,
Polypropylene with 20% Glass Fiber Filler
,
Polypropylene with 20% Talc Filler
,
Polypropylene with 30% Talc Filler
,
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
,
Polypropylene, Flame Retardant
,
Polypropylene with 10% Glass Fiber Filler
,
Polypropylene with 30% Glass Fiber Filler
,
Polypropylene Copolymer
,
Polypropylene with 10% Talc Filler
,
Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
,
Polypropylene, Blow Molding Grade
,
Polypropylene, Extrusion Grade
,
Polypropylene, Mineral Reinforced
,
Film
,
Polypropylene with 50% Calcium Carbonate
,
Polypropylene, Film Grade
Manufacturer
Inno-Comp Ltd
Tips:
Up to 50 items displayed.
PRODUCT NO.
Category
Inno-Comp INNOPOL® CS 1-2820 20% Glass-Fibre-Filled Polypropylene Homopolymer
Polypropylene with 20% Glass Fiber Filler
Inno-Comp INNOPOL® CS 1-3000 B DEL Polypropylene Homopolymer
Polypropylene (PP)
Inno-Comp INNOPOL® CS 1-3120 B DEL 20% Talc Filled Polypropylene Homopolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 1-3120 N DEL 20% Talc Filled Polypropylene Homopolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 1-3130 30% Talc-Filled Polypropylene Homopolymer
Polypropylene with 30% Talc Filler
Inno-Comp INNOPOL® CS 1-3140 40% Talc-Filled Polypropylene Homopolymer
Polypropylene with 40% Talc Filler
Inno-Comp INNOPOL® CS 1-3250 42% Chalk-Filled Polypropylene Homopolymer
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Inno-Comp INNOPOL® CS 1-3260 55% Chalk-Filled Polypropylene Homopolymer
Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Inno-Comp INNOPOL® CS 1-3610 UW Polypropylene Homopolymer
Polypropylene, Flame Retardant
Inno-Comp INNOPOL® CS 1-3810 10% Glass-Fiber-Filled Polypropylene Homopolymer
Polypropylene with 10% Glass Fiber Filler
Inno-Comp INNOPOL® CS 1-3820 20% Glass-Fiber-Filled Polypropylene Homopolymer
Polypropylene with 20% Glass Fiber Filler
Inno-Comp INNOPOL® CS 1-3830 30% Glass-Fiber-Filled Polypropylene Homopolymer
Polypropylene with 30% Glass Fiber Filler
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer
Polypropylene with 40% Talc Filler
Inno-Comp INNOPOL® CS 1-5120 BLH 20% Talc-Filled Polypropylene Homopolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer
Polypropylene with 40% Talc Filler
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer
Polypropylene with 20% Glass Fiber Filler
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer
Polypropylene with 40% Talc Filler
Inno-Comp INNOPOL® CS 1-8000 Polypropylene Homopolymer
Polypropylene (PP)
Inno-Comp INNOPOL® CS 2-1000 Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-2000 TO Polypropylene Block-Copolymer Based Compound
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-2110 10% Talc-Filled Polypropylene Block-Copolymer
Polypropylene with 10% Talc Filler
Inno-Comp INNOPOL® CS 2-2120 17TOP BU UV-Stabilized 17% Talc-Filled Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-2120 20% Talc-Filled Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-3000 Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-3120 20% Talc Filled Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-3120 BPLU 9H0017 20% Talc-Filled, UV Stabilized Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-3130 NU UV-Stabilized 30% Talc-Filled Polypropylene Block-Copolymer
Polypropylene with 30% Talc Filler
Inno-Comp INNOPOL® CS 2-3302 Elastomer Modified Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-3302 TO BU Elastomer Modified, UV-Stabilized Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-3522 TO BU 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-4210 10% Chalk-Filled Polypropylene Block-Copolymer
Polypropylene with 10% Calcium Carbonate (CaCO3) Filler
Inno-Comp INNOPOL® CS 2-4630 GFR Flame Retarded Polypropylene Block-Copolymer
Polypropylene, Flame Retardant
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-8302 Elastomer Modified Polypropylene Block-Copolymer
Polypropylene, Blow Molding Grade
Inno-Comp INNOPOL® CS 2-8960 60% Barium-Sulfate Filled Polypropylene Block-Copolymer
Polypropylene, Extrusion Grade
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-9000 Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-9110 10% Talc-Filled Polypropylene Block-Copolymer
Polypropylene with 10% Talc Filler
Inno-Comp INNOPOL® CS 2-9120 20% Talc-Filled Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-9301 Elastomer Modified Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-9302 Elastomer Modified Polypropylene Block-Copolymer
Polypropylene Copolymer
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
Polypropylene with 10% Talc Filler
Inno-Comp INNOPOL® CS 2-9523 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 2-9524 20% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 3-3120 B 20% Talc-Filled Polypropylene
Polypropylene with 20% Talc Filler
Inno-Comp INNOPOL® CS 3-9230 KAR BU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer
Polypropylene, Mineral Reinforced
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer
Polypropylene, Mineral Reinforced
Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene
Polypropylene, Film Grade
Inno-Comp INNOPOL® CS 1-1120 AN 20% Talc-Filled Polypropylene Homopolymer
Polypropylene with 20% Talc Filler