| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded |
| Manufacturer | Star Plastics, Inc |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Star Plastics ABS5035 Molding Grade ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.05 g/cc | 1.05 g/cc | ASTM D792 |
| Maximum Moisture Content | 0.15 | 0.15 | |
| Linear Mold Shrinkage | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
| Melt Flow | 5.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 40.0 MPa | 5800 psi | ASTM D638 |
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
| Flexural Yield Strength | 58.6 MPa | 8500 psi | ASTM D790 |
| Flexural Modulus | 2.07 GPa | 300 ksi | ASTM D790 |
| Izod Impact, Notched | 1.87 J/cm | 3.50 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 76.7 °C | 170 °F | unannealed, .125in; ASTM D648 |
| Flammability, UL94 | HB | HB |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 188 - 218 °C | 370 - 425 °F | |
| Middle Barrel Temperature | 204 - 232 °C | 400 - 450 °F | |
| Front Barrel Temperature | 218 - 246 °C | 425 - 475 °F | |
| Nozzle Temperature | 218 - 274 °C | 425 - 525 °F | |
| Melt Temperature | 218 - 274 °C | 425 - 525 °F | |
| Mold Temperature | 48.9 - 76.7 °C | 120 - 170 °F | |
| Drying Temperature | 82.2 - 93.3 °C | 180 - 200 °F | |
| Dry Time | 2 - 4 hour | 2 - 4 hour | |
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
| Screw Speed | 25 - 75 rpm | 25 - 75 rpm |