| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Plaskolite West Optix® CA-990 Impact Modified Acrylic Resin
Injection Molding and Extrusion Grade. Excellent surface gloss.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
Radici Radilon® S ESL128 (dry) Nylon 6
Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
|
Lanxess Durethan® DP 2325 H3.0 DUS031 000000 Nylon 66
PA 66, non-reinforced, injection molding, improved flowability, impact modified, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
|
Lanxess Pocan® S 1517 000000 PBT
PBT, non-reinforced, injection molding, extrusion, impact modified
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527-1,-2 |
|
Ineos ABS Lustran® Ultra 4105 ABS Pellets (Polycarbonate-modified), Medium High Heat Grade
Lustran® Ultra 4105 is medium high heat grade with superior impact resistance. It is PC-modified and has low emission. It is used for the production of molded plastic articles.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 221 PA66, Conditioned
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA12 (Europe-Africa-Middle East)
LNP* LUBRICOMP* SP003 is a compound based on PA 12 resin containing PTFE/Silicone. Added features include: Internally Lubricated.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRILOY D20001 PPO
LNP* LUBRILOY* Z20001 is a compound based on PPO resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 5 mm/min; ASTM D 638 |
|
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific)
Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xylex X7200 PC+POLYESTER (Europe-Africa-Middle East)
General purpose, UV stabilised Xylex gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East)
Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP Thermocomp FX05032 PE (Europe-Africa-Middle East)
LNP* THERMOCOMP* FX05032 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added features include : Foaming Agent for Polyolefins.This data was supplied by SABIC-IP for t..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D 638 |
|
Styrolution PS 6220 HIPS
Excellent toughnessHigh glossDesigned for deep draw thermoformingInformation provided by Styrolution
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1mm/min; ISO 527 |
|
Styrolution Terblend® N NM-19 ABS/PA6 (Dry)
Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROL..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1mm/min; ISO 527 |
|
Styrolution Terlux® 2802 TR MABS
Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 50 mm/min; ASTM D638 |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Tensile Modulus | 2.00 - 2.20 GPa | 290 - 319 ksi | MD; ISO 527-2 |
|
Borealis HC101BF Polypropylene Homopolymer
HC101BF is a polypropylene homopolymer. Applications: HC101BF has been developed especially for applications like: co-extrusion applications, print lamination, metallisable film, coated film, packa..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Total PS CPDS 822 Standard Flow, Non-Deca Polystyrene
Total Petrochemicals Polystyrene 822 is a good flow, environmentally friendly high impact Polystyrene for injection molding. It is recommended for the manufacturing of articles which require good d..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
Covestro Bayblend® T 44 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 45 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® L 20 LF grey PA12
Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
|
Eurotec® Tecomid® NB40 NL IL PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
BASF Procom® D 1189 Polypropylene
Data was collected by ISO methods and provided by BASF.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Americas Styrenics STYRON® 478 High Impact Polystyrene
Product CharacteristicsGood glossExcellent balance of flow and stiffnessFood Contact CompliantUL Classification 94HBUSP Class VITypical ApplicationsAppliancesMedicalHousewaresConsumer electronicsIn..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min |
|
Arkema Group Kynar® 1000 HDC N 118 PVDF
(discontinued **)
Designation ISO 12086-PVDF-E,GG1C,P.?E5.I.B.E.C,, ?(1.5-2.5)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, hig..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-2 |
|
Total Lacqrene® 6630 Impact Polystyrene
(discontinued **)
LACQRENE® 6630 and 6631 are easy flowing, high impact polystyrenes for injection molding. With easy processing, good rigidity and ease of coloration. These grades find a wide range of application..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
ExxonMobil Paxon™ AS55-003 Blow Molding Resin
(discontinued **)
AS55-003 is a blow molding grade high density polyethylene copolymer containing an antistat additive. It provides a good balance of stiffness and stress crack resistance.Information provided by Exx..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
ExxonMobil Paxon™ AU55-003 Blow Molding Resin
(discontinued **)
AU55-003 is a blow molding grade high density polyethylene containing an excellent antistat additive, offering a good combination of stiffness and stress crack resistance. An enhanced additive pack..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
|
Polyram RamSter PF801 PBT, High Impact Modified
High impact modified PBT for injection molding applications.Information provided by Polyram.
|
|||