| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Modulus | 2.00 GPa | 290 ksi | STN EN ISO 527-2 |
|
Plastcom PLASTAMID® 6 BT N 26 B PA6
Basic type PA 6 for compounding, for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in the natural mode and in the full RAL color scale.Information Prov..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-2 |
|
Total Lacqrene® 3351(EU) Impact Polystyrene
(discontinued **)
LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min |
|
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
(discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM-D638 |
|
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Ineos Nova FX530 Impact Polystyrene
Features: Excellent environmental stress crack resistanceExcellent Izod impact strengthUL Classification 94 HBBalanced physical propertiesApplications: ExtrusionThermoformingSelected injection moldi..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
|
Lanxess Pocan® S 1517 000000 PBT
PBT, non-reinforced, injection molding, extrusion, impact modified
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® A 221 PA66, Conditioned
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 Type 1A |
|
Solvay TECHNYL® C 246 M PA6, DRY
Description: Unreinforced polyamide 6, with high impact resistance, for injection molding. Grade formerly known as PSB196.Available in: EuropeProduct Applications: It is particularly adapted to the ..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics Xylex X7200MR PC+POLYESTER (Europe-Africa-Middle East)
Mold Release version of X7200This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
|
Styrolution Polystyrol 495 F GR 2 PS
Description: Polystyrol 495 F is a high impact polystyrene with a good heat resistance and high stiffness.Applications: Consumer electronics; TV-front and back; chassis for VCR and CD player. Househ..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | At 1 mm/min; ISO 527-2 |
|
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications
Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | dry; ISO 527 |
|
Ter Hell Plastic K-Resin KRE 9902 Butadiene-Styrene Copolymer
Description: Butadiene-Styrene Copolymer Compound, good transparency with impact strength and stiffness well-balanced.Application: For all kinds of injection molded parts.Information provided by T..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
|
Polyram PlusTek PB340S50 Nylon 6 for Injection Molding, 50% Glass-beads Reinforced, Heat Stabilized
50% Glass-beads reinforced, heat stabilized Nylon 6 for injection molding applications.Information provided by Polyram.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM-D790 |
|
Polyram RamOfin PPC371B73 Polypropylene, 73% Mineral Filled
73% mineral filled polypropylene for heavy density injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
|
Eastman Drystar 0325 Copolyester
This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
Covestro Bayblend® T 44 Polycarbonate/ABS Blend
Easier flowing than BAYBLEND T 45 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
Covestro Baydur® 110 FR Polyurethane
Rigid microcellular RIM polyurethane material. Fast demold times; self releasing; long flow paths possible, therefore suitable for production of large moldings. Parts are injected through only one ..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | conditioned; ISO 527-1/-2 |
|
EMS-Grivory Grivory® AS V0 PA66
Product description: Grilon AS V0 is an unreinforced, normal viscosity, self-extinguishing PA66 injection molding grade. Grilon AS V0 has the following important properties: Halogen and phosphorous-..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | chs 2.0 in/min; ASTM D638 |
|
Diamond Polymers Centrex® 813 General Purpose Injection Molding Grade ASA/AES
Centrex 813 resin is a high-gloss, high-impact grade of ASA/AES, a blend of acrylonitrile-styrene-acrylate and acrylonitrile-ethylene-propylene styrene. This injection molding grade with a good bala..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-2 |
|
Domo 1040RC Polypropylene Homopolymer
Information provided by Domo.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
|
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural
Information provided by Eurotec®
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527-1/-2 |
|
DSM Arnite® B604T PBT-I |
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ISO 527 |
|
Eurotec® Tecomid® NB40 NL IL PA 6 impact modified
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Azdel SuperLite® SL550700-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness)
AZDEL SuperLite® SL550700-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | ASTM D638 |
|
Azdel SuperLite® SL551000-100 PP Resin Matrix / 55% Glass Fiber (3.5 mm Molded Thickness)
AZDEL SuperLite® SL551000-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
BASF Novolen® 1040 N Polypropylene
Nucleated grade for injection molded parts.Data was collected by ISO methods and provided by BASF.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | 1 mm/min; ISO 527 |
|
SABIC Innovative Plastics LNP LUBRICOMP CL002 PS (Europe-Africa-Middle East)
LNP* LUBRICOMP* CL002 is a compound based on Polystyrene resin containing PTFE. Added features include: Internally Lubricated.
|
|||
| Tensile Modulus | 2.00 GPa | 290 ksi | |
|
LATI Latishield 52/5-07A PP Homopolymer, Steel Fiber Reinforced
EMI shielding product based on Polypropylene homopolymer (PPh). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
|
|||