| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
PlastiComp Complet® LCF50 - PA6 Nylon 6, 50% Long Carbon Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% carbon fiber reinforcementInformation provided by PlastiComp, Inc.
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
PlastiComp Complet® LGF40 - PA66 MT Nylon 66, 40% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementImpact modifiedInformation provided by..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
LG Chemical Lupox® PBT-GP-1000 High Flow PBT
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Fiberfil® J-69/20/E High performance polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP 1166B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1579C Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1580L1-UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1627I Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1736S Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1829-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1871 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1880 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1900-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-1959G Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2197 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2207 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2239 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP 1128 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2676 UV Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® OBC 4773A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-1000-105UV Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-1524E Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-2363B Thermoplastic Elastomer
Availability: North America Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weath..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-2555F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-2560A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-2585A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Teknor Apex Telcar® TL-355 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
|
|||
| Back Pressure | 0.172 - 0.345 MPa | 25.0 - 50.0 psi | |
|
Clariant 66G43HLS-Black Nylon 66, 43% Glass Fiber Reinforced, Heat Stabilized, Lubricated
Data provided by Clariant Masterbatches
|
|||
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
|
Teknor Apex Monprene® MP-2730 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
|
|||