Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc | ASTM D792 |
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
Water Absorption at Saturation | 0.35 % | 0.35 % | ISO 62 |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0080 in/in @Thickness 0.126 in |
SABIC Method |
Melt Flow | 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
17 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Melt Index of Compound | 16 g/10 min @Load 1.20 kg, Temperature 300 °C |
16 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 95.0 MPa | 13800 psi | ISO 2039-1 |
Tensile Strength at Break | 55.0 MPa | 7980 psi | 50 mm/min; ISO 527 |
58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 | |
Tensile Strength, Yield | 58.0 MPa | 8410 psi | Type I, 50 mm/min; ASTM D638 |
59.0 MPa | 8560 psi | 50 mm/min; ISO 527 | |
Elongation at Break | 100 % | 100 % | 50 mm/min; ISO 527 |
103 % | 103 % | Type I, 50 mm/min; ASTM D638 | |
Elongation at Yield | 5.0 % | 5.0 % | 50 mm/min; ISO 527 |
5.8 % | 5.8 % | Type I, 50 mm/min; ASTM D638 | |
Tensile Modulus | 2.20 GPa | 319 ksi | 1 mm/min; ISO 527 |
2.26 GPa | 328 ksi | 50 mm/min; ASTM D638 | |
Flexural Yield Strength | 88.0 MPa | 12800 psi | 2 mm/min; ISO 178 |
95.0 MPa | 13800 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
2.33 GPa | 338 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
Izod Impact, Notched | 7.31 J/cm | 13.7 ft-lb/in | ASTM D256 |
5.60 J/cm @Temperature -30.0 °C |
10.5 ft-lb/in @Temperature -22.0 °F |
ASTM D256 | |
Izod Impact, Notched (ISO) | 55.0 kJ/m² | 26.2 ft-lb/in² | 80*10*3; ISO 180/1A |
20.0 kJ/m² @Temperature -30.0 °C |
9.52 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
NB @Temperature -30.0 °C |
NB @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
Charpy Impact, Notched | 6.00 J/cm² | 28.6 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
2.50 J/cm² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
Dart Drop, Total Energy | 67.0 J @Temperature 23.0 °C |
49.4 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
40.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
75.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
41.7 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 | |
Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | 277 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
136 °C @Thickness 3.20 mm |
277 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Deflection Temperature at 1.8 MPa (264 psi) | 124 °C | 255 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
123 °C @Thickness 3.20 mm |
253 °F @Thickness 0.126 in |
unannealed; ASTM D648 | |
Vicat Softening Point | 143 °C | 289 °F | Rate B/50; ASTM D1525 |
143 °C | 289 °F | Rate B/50; ISO 306 | |
144 °C | 291 °F | Rate B/120; ISO 306 | |
UL RTI, Electrical | 50.0 °C | 122 °F | UL 746B |
UL RTI, Mechanical with Impact | 50.0 °C | 122 °F | UL 746B |
UL RTI, Mechanical without Impact | 50.0 °C | 122 °F | UL 746B |
Flammability, UL94 | V-0 @Thickness 1.50 mm |
V-0 @Thickness 0.0591 in |
UL 94 |
5VA @Thickness 3.00 mm |
5VA @Thickness 0.118 in |
UL 94 | |
Oxygen Index | 40 % | 40 % | ISO 4589 |
Glow Wire Test | 825 °C | 1520 °F | IEC 60695-2-13 |
960 °C @Thickness 1.00 mm |
1760 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Constant | 2.7 @Frequency 1.00e+6 Hz |
2.7 @Frequency 1.00e+6 Hz |
IEC 60250 |
2.7 @Frequency 50.0 - 60.0 Hz |
2.7 @Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
Dielectric Strength | 19.0 kV/mm @Thickness 3.20 mm |
483 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Dissipation Factor | 0.00040 @Frequency 50.0 - 60.0 Hz |
0.00040 @Frequency 50.0 - 60.0 Hz |
IEC 60250 |
0.010 @Frequency 1.00e+6 Hz |
0.010 @Frequency 1.00e+6 Hz |
IEC 60250 | |
Comparative Tracking Index | 175 V | 175 V | IEC 60112 |
Descriptive Properties | Value | Comments |
---|---|---|
Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |