| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Asia Pacific)
Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1...
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS
Reinforced PC/ABS with high stiffness and low CTE.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® XCM850 PC+ABS (Asia Pacific)
Reinforced PC/ABS with high stiffness and low CTE.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® XP7560 ASA (Europe-Africa-Middle East)
GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours.
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific)
Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent ..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics GELOY XP7560 ASA (Europe-Africa-Middle East)
GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours.
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXL9132 PC Copolymer (Europe-Africa-Middle East)
Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temperature ductility, UV stabilized. Non-chlorinated, non-brominated flame retardant product. UL rated V0/5VA.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HFD4271 PC
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East)
NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/1eA |
|
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, Conditioned
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Europe-Africa-Middle East)
LNP* Lubricomp* Lexan_WR2210 compound is based on an aternative polymeric wear technology and does not contain silicones. LEXAN WR2210 has superior processability (flow similar to LEXAN 121) and par..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4mm, Cut; ISO 180/1A |
|
SABIC Innovative Plastics SABIC PPCOMPOUND 7705 PP
SABIC® PPcompound 7705 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, scratch resistance, and heat stability with interior automotive UV stabili..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East)
VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin.
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xenoy® HX6600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX6600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xenoy® IQ4840 PBT+PC (Europe-Africa-Middle East)
Xenoy iQ4840 (PBT+PC) resin is an environmental responsible, sustainable, and low carbon footprint resin. It is a 10% mineral filled resin with high modulus and ductile (HMD) characteristics. Xen..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP PF1006HI005 PA 6 (Europe-Africa-Middle East)
High Impact Nylon 6 compound containing Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP VERTON MV007U PP (Europe-Africa-Middle East)
LNP* VERTON* MV007U is a compound based on PP resin containing Long Glass Fiber. Added features include; Chemically Coupled, Heat Stabilized, UV Stabilized.
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL GTX GTX964 PPE+PA (Europe-Africa-Middle East)
NORYL GTX964 is an unfilled impact modified material with optimised processability.
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature -30.0 °C |
9.52
ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature 0.000 °C |
9.52
ft-lb/in² @Temperature 32.0 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific)
Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180 |
|
Polyram PlusTek PA862 Nylon 6.6 for Injection Molding, High Impact Modified
High impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ISO 180/1A |
|
DSM Stanyl® TE263F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Impact Modified (North America)
Information provided by DSM Engineering Plastics.
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 50%RH; ISO 180/1A |
|
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**)
30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | 80x10x4; ISO 180/1A |
|
Eurostar Starpylen MZ006S PP, Glass Fiber Filled, Injection Molded
Starpylen MZ006S is a Glass fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WT 30GF S3)Information provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
20.0
kJ/m² @Temperature 23.0 °C |
9.52
ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Thermotuf WF006I Polyester, TP
LNP THERMOTUF* WF006I is a compound based on Polyester, TP resin containing Glass Fiber. Added features of this material include: High Impact.This data was supplied by SABIC-IP for the Americas reg..
|
|||
| Izod Impact, Notched (ISO) | 20.0 kJ/m² | 9.52 ft-lb/in² | ASTM D256 |
|
Tipco Tipcolene® IA 933 IN - 20% Talc/Mineral Reinforced Polypropylene Copolymer, High Flow, Stiffness & Impact Strength
20% Mineral Reinforced, High Stiffness, High Impact PP CopolymerApplications: Automotive InteriorsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India...
|
|||