| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | Lexan® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.29 g/cc | 1.29 g/cc | ASTM D792 |
| Density | 1.29 g/cc | 0.0466 lb/in³ | ISO 1183 |
| Water Absorption | 0.15 % <br>@Time 86400 sec |
0.15 % <br>@Time 24.0 hour |
ASTM D570 |
| Moisture Absorption | 0.150 % | 0.150 % | 23°C / 50% RH; ISO 62 |
| Water Absorption at Saturation | 0.35 % | 0.35 % | ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
| 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method | |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.20 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.126 in |
SABIC Method |
| Melt Flow | 32 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
32 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
ASTM D1238 |
| Melt Index of Compound | 30 g/10 min <br>@Load 1.20 kg,<br> Temperature 300 °C |
30 g/10 min <br>@Load 2.65 lb,<br> Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, H358/30 | 105 MPa | 15200 psi | ISO 2039-1 |
| Tensile Strength at Break | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D638 |
| 52.0 MPa | 7540 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | 50 mm/min; ISO 527 |
| 60.0 MPa | 8700 psi | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Break | 70 % | 70 % | 50 mm/min; ISO 527 |
| 80 % | 80 % | Type I, 50 mm/min; ASTM D638 | |
| Elongation at Yield | 5.0 % | 5.0 % | 50 mm/min; ISO 527 |
| 5.0 % | 5.0 % | Type I, 50 mm/min; ASTM D638 | |
| Tensile Modulus | 2.35 GPa | 341 ksi | 1 mm/min; ISO 527 |
| 2.50 GPa | 363 ksi | 5 mm/min; ASTM D638 | |
| Flexural Yield Strength | 90.0 MPa | 13100 psi | 2 mm/min; ISO 178 |
| 93.0 MPa | 13500 psi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
| 2.45 GPa | 355 ksi | 1.3 mm/min, 50 mm span; ASTM D790 | |
| Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | NB | NB | ASTM D4812 |
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*3; ISO 180/1A |
| 10.0 kJ/m² <br>@Temperature -30.0 °C |
4.76 ft-lb/in² <br>@Temperature -22.0 °F |
80*10*3; ISO 180/1A | |
| Izod Impact, Unnotched (ISO) | NB | NB | 80*10*3; ISO 180/1U |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
80*10*3; ISO 180/1U | |
| Charpy Impact Unnotched | NB | NB | Edgew 80*10*3 sp=62mm; ISO 179/1eU |
| NB <br>@Temperature -30.0 °C |
NB <br>@Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eU | |
| Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
| 1.10 J/cm² <br>@Temperature -30.0 °C |
5.23 ft-lb/in² <br>@Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA | |
| Dart Drop, Total Energy | 55.0 J <br>@Temperature 23.0 °C |
40.6 ft-lb <br>@Temperature 73.4 °F |
ASTM D3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 70.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
ASTM D696 |
| 70.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| CTE, linear, Transverse to Flow | 70.0 µm/m-°C <br>@Temperature -30.0 - 30.0 °C |
38.9 µin/in-°F <br>@Temperature -22.0 - 86.0 °F |
ASTM D696 |
| 70.0 µm/m-°C <br>@Temperature 23.0 - 80.0 °C |
38.9 µin/in-°F <br>@Temperature 73.4 - 176 °F |
ISO 11359-2 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 133 °C | 271 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 125 °C <br>@Thickness 3.20 mm |
257 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 122 °C | 252 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 127 °C <br>@Thickness 3.20 mm |
261 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Vicat Softening Point | 138 °C | 280 °F | Rate B/50; ASTM D1525 |
| 139 °C | 282 °F | Rate B/50; ISO 306 | |
| 141 °C | 286 °F | Rate B/120; ISO 306 | |
| UL RTI, Electrical | 80.0 °C | 176 °F | UL 746B |
| UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
| UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
| Flammability, UL94 | V-2 <br>@Thickness 0.750 mm |
V-2 <br>@Thickness 0.0295 in |
UL 94 |
| V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
UL 94 | |
| Oxygen Index | 36 % | 36 % | ISO 4589 |
| Glow Wire Test | 850 °C | 1560 °F | IEC 60695-2-13 |
| 960 °C <br>@Thickness 1.00 mm |
1760 °F <br>@Thickness 0.0394 in |
IEC 60695-2-12 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm | ROA; IEC 60093 |
| Dielectric Constant | 3.2 <br>@Frequency 1.00e+6 Hz |
3.2 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.2 <br>@Frequency 50.0 - 60.0 Hz |
3.2 <br>@Frequency 50.0 - 60.0 Hz |
IEC 60250 | |
| Dielectric Strength | 21.0 kV/mm <br>@Thickness 1.60 mm |
533 kV/in <br>@Thickness 0.0630 in |
in oil; ASTM D149 |
| Dissipation Factor | 0.010 <br>@Frequency 50.0 - 60.0 Hz |
0.010 <br>@Frequency 50.0 - 60.0 Hz |
IEC 60250 |
| 0.010 <br>@Frequency 1.00e+6 Hz |
0.010 <br>@Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 225 V | 225 V | IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Ball Pressure Test, 125°C +/- 2°C | PASSES | IEC 60695-10-2 |