Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : UL RTI, Mechanical with Impact = 176 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Cycoloy® C1200HFM PC+ABS (Asia Pacific)
PC+ABS-MAGIX version in various metallic colors. High heat/good flow characteristics. Appliances, automotive/telecommunication.
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Cycoloy® FXC810AR PC+ABS (Europe-Africa-Middle East)
CYCOLOY FXC810AR is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Ares colour effects. The colour package may effect performance.This data was supplie..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East)
High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® BFL2000 PC (Asia Pacific)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® BX9349 PC COPOLYMER (Asia Pacific)
Lexan* BX9349 resin is an injection moldable modified PC resin with non-brominated and non-chlorinated flame retardant to meet UL-94 V0 at 0.5mm and V2 at 0.4mm. Balanced flow with low temperature d..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746
Polymer Resources PC-BR1-UV Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilized
Polycarbonate, Branched for Extrusion and Blow Molding, UV-stabilizedFeatures: • Ultra High Impact Resistance • Ultra High ViscosityProcess: Extrusion/Blow MoldingNotes: All physical, mechanical..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® EXL6414 PC (Asia Pacific)
PC-Siloxane copolymer with excellent processability. Impact modified, medium flow, extreme low temp. ductility.
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® FL903 PC
Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized.
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East)
LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® ML3513 PC (Europe-Africa-Middle East)
LEXAN ML3513 is a high viscosity, 30% short fibre glass reinforced, flame retardant grade, especially designed for connectors and relay separators.This data was supplied by SABIC-IP for the Europe-A..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® FL2003 PC (Asia Pacific)
Various weight reductions at 0.250" (6.35mm) wall. Low temperature impact and high heat resistant. Excellent surface. UV-stabilized.This data was supplied by SABIC-IP for the Asia Pacific region...
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® FL403 PC
Various weight reductions at 0.250"" wall. UV-resistant. Impact resistant, Superior processing, excellent surface. UL94 V-0/5V at 0.125"".
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East)
Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® ML3041 PC (Europe-Africa-Middle East)
LEXAN ML3041 has been developed for the injection moulding of thin-wall, complex parts that require high mechanical properties and impact resistance.This data was supplied by SABIC-IP for the Europe..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.500 - 2.50 mm
176 °F

@Thickness 0.0197 - 0.0984 in
LG Chemical Lupoy 3010-22 Polycarbonate Resin
Description: LUPOY PC 3010-22 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness >=0.700 mm
176 °F

@Thickness >=0.0276 in
LG Chemical LUPOY SC1004A PC
Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 0.500 - 2.50 mm
176 °F

@Thickness 0.0197 - 0.0984 in
LG Chemical Lupoy 3010-30 Polycarbonate Resin
Description: LUPOY PC 3010-30 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC
LNP* Lubricomp* Lexan_LF1510A compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances.
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.47 mm
176 °F

@Thickness 0.0579 in
UL 746B
Teijin Panlite® LN-1010RM High Light Reflection, Flame Resistant Polycarbonate Resin
Polycarbonate-resin-base flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even at a thinner th..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics NORYL PX1007 PPE+PS
Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade.
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
Covestro Makrolon® FR6901 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Hig..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 3.20 mm
176 °F

@Thickness 0.126 in
UL746B
Covestro Prism® CM-200 Polyurethane Solid RIM, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o..
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.50 mm
176 °F

@Thickness 0.0591 in
UL 746B
Diamond Polymers ABS 9502
Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc.
UL RTI, Mechanical with Impact 80.0 °C

@Thickness 1.47 mm
176 °F

@Thickness 0.0579 in
UL 746B
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin
CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® HFD4271 PC (Europe-Africa-Middle East)
Lexan* HFD4271 is a 10% glass filled, high flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4271 has enhanced mold release, impact ductility..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® HFD4471 PC (Asia Pacific)
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Lexan® HFD4471 PC (Europe-Africa-Middle East)
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..
UL RTI, Mechanical with Impact 80.0 °C
176 °F
UL 746B
SABIC Innovative Plastics Noryl EN212 PPE+PS
Extrusion grade. 212F (100C) DTUL. UL94 V-1 rated.This data was supplied by SABIC-IP for the Americas region.