Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 3011ZD86 Tungsten Filled Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ecomass® 3011ZD86 Tungsten Filled Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 6.00 g/cc
6.00 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa
3920 psi
ISO 527
Elongation at Break <= 5.0 %
<= 5.0 %
ISO 527
Flexural Strength 35.0 MPa
5080 psi
ISO 178
Flexural Modulus 5.92 GPa
859 ksi
ISO 178
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180-A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 270 - 315 °C
518 - 599 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 121 °C
250 °F
Dry Time 3 - 4 hour
3 - 4 hour