| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® 223R PC
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h..
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPH4504HEU PPC (Europe-Africa-Middle East)
High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, ..
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LI1813R PC (Europe-Africa-Middle East)
Low-viscosity multi-purpose PC having low levels of ionics species. UV-stabilized.
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LUX2114 PC (Asia Pacific)
18 MFR. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East)
Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope..
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific)
10 MFR. Improved flame retardance. Internal mold release. UV stabilized.
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature -30.0 °C
|
5.23
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® OQ1022 PC
Standard Flow OQ Resin
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP FARADEX DS0036I PC
LNP* FARADEX* DS0036I is a compound based on Polycarbonate resin containing 15% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, No..
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP FARADEX NX07330 PC+ABS (Asia Pacific)
Faradex NX07330 is a compound based on PC+ABS blend resin containing stainless steel and glass fiber. Added features of this material include EMI/RFI Shielding and ESD.
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature 23.0 °C
|
5.23
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**)
Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a..
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® BFL2000U PC (Europe-Africa-Middle East)
Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig..
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® ML3732 PC (Europe-Africa-Middle East)
Lexan ML3732 is a low viscosity flame retardant grade, especially designed to pass the glow wire test according EDF HN60-S-02 at a thickness of 3.2 mm.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP DFL349 PC
LNP LUBRICOMP* DFL349 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Flame Retardant, Internally Lubricated.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | |
|
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled
Crystalline Polymer Blend, Glass Filled, Impact Modified
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC
LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | ISO 180/1eA |
|
Solvay TECHNYL® A 218G V30 PA66, 30% glass fiber, DRY
Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding specially stabilized to improve its resistance automotive cooling liquids.Available in: Europe and Latin Americ..
|
|||
| Izod Impact, Notched (ISO) |
11.0
kJ/m² <br>@Temperature 23.0 °C
|
5.23
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP Lubricomp UFL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36ASP is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE.
Added features include Internally Lubricated, Heat Stabilized.This data was supplied by SABIC-IP f..
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific)
LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK
LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK
LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics LNP THERMOCOMP UF007SXC PPA (Europe-Africa-Middle East)
LNP* THERMOCOMP* UF007SXC is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include : Heat Stabilized .
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL FXN121LG PPE+HIPS
Noryl* FXN121LG is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | Conditioned; ISO 180/1A |
|
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled
Glass fiber reinforced, high strengthInformation provided by Addiplast.
|
|||
| Izod Impact, Notched (ISO) | 11.0 kJ/m² | 5.23 ft-lb/in² | 80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics NORYL FXN119BK PPE+HIPS (Asia Pacific)
Noryl* FXN119BK is a low gloss PPE/HIPS grade. It provides a balance of mechanical properties and heat performance with intrinsic low gloss appreance. FXN119BKBK is available in black only.
|
|||