Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL903 PC Various weight reductions at 0.250"" (6.35 mm). High heat/creep resistance, excellent impact, flexural strength/rigidity. UV-stabilized. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3412HF PC 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | |
PTS Tristar® PC-10GFR 10% Glass Reinforced Polycarbonate With Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FXM941A PC PC in special effects colors. Metallic and pearlescent additives. Color package may affect performance. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4211 PC (Europe-Africa-Middle East) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Mechanical without Impact | 80.0 - 130 °C | 176 - 266 °F | Average value: 107 °C Grade Count:13 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3010-10 Polycarbonate Resin Description: LUPOY PC 3010-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3030-10 Polycarbonate Resin Description: LUPOY PC 3030-10 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 0.500 - 2.50 mm |
176 °F @Thickness 0.0197 - 0.0984 in |
|
LG Chemical Lupoy 3030-15 Polycarbonate Resin Description: LUPOY PC 3030-15 resin is designed for injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Character.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | |
LG Chemical LUPOY SR3108L PC, High Impact Description: Injection Molding, PC, High Flow, High Impact, White Color OnlyApplication: BLU Mold frame for Mobile DevicesCAS: 103598-77-2 and 13463-67-1Information provided by LG Chemical |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Asia Pacific) 10% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1510 compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics NORYL GN390 PPE+PS (Asia Pacific) Closed loop recycle grade for CANON, 13% PCR-PS loaded, HDT 90C, V-0/1.2mm |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
|
Covestro Bayblend® FR 90 N Polycarbonate/ABS Blend Flame retardant grade with antimony, chlorine and bromine free, flame retardant package, optimized processability.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sepa.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® FR 7067 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® FR 7087 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 1002 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 7602B Description: Blow Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® BN-8120R Improved Mold Release, Carbon Fiber Reinforced, Flame Resistant Polycarbonate Resin CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are flame retardance, low molding shrinkage and dimensiona.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C @Thickness 5.99 mm |
176 °F @Thickness 0.236 in |
UL 746 |
Polymer Resources PCSF-FR1 Polycarbonate, 10% Glass Reinforced Structural Foam Grade Polycarbonate, 10% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4412 PC (Asia Pacific) Lexan* HFD4412 is a 20% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Mechanical without Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East) LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow. |