Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Index of Compound = 30 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 230 °C
30 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Polykemi AB POLYabs SS0 GK10 ABS, High Flow
Information provided by Polykemi AB
Melt Index of Compound 30 g/10 min

@Load 10.0 kg,
Temperature 220 °C
30 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Polykemi AB POLYasa 3010F Extra High Flow ASA
Information provided by Polykemi AB
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Polykemi AB POLYblend 50LG PC/ABS-Blend, Low Gloss
Information provided by Polykemi AB
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 260 °C
30 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific)
Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat..
Melt Index of Compound 30 g/10 min

@Load 1.20 kg,
Temperature 300 °C
30 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® BFL2000 PC
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Melt Index of Compound 30 g/10 min

@Load 1.20 kg,
Temperature 300 °C
30 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® ML7677 PC (Asia Pacific)
Transparent Polycarbonate in limited colors. Excellent processability, super high flow, flame retardant, UL rated V-1 at 2.0mm
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 330 °C
30 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 330 °C
30 g/10 min

@Load 4.76 lb,
Temperature 626 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific)
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Index of Compound 30 g/10 min

@Load 1.20 kg,
Temperature 300 °C
30 g/10 min

@Load 2.65 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East)
Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors.
Melt Index of Compound 30 g/10 min

@Load 21.6 kg,
Temperature 190 °C
30 g/10 min

@Load 47.6 lb,
Temperature 374 °F
cm<sup>3</sup>/10 min
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t..
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
MVR, [cm<sup>3</sup>/10 min]
Huntsman IROGRAN® A 70 H 4714 M TPU-Polyester
Introduction: IROGRAN A 70 H 4714 M is a soft polyester based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 70 H 4714 M is part of the HUNTSMAN injection molding ..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 260 °C
30 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Mitsui APELâ„¢ APL6509T Cyclo Olefin Copolymer (COC)
This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces..
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 260 °C
30 g/10 min

@Load 11.0 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL RN0401 PPE+PS
Noryl RN0401 resin is an unfilled Post Consumer Recycle (PCR) based injection moldable modified polyphenylene ether blend comprising at least 20% PCR content. Available in black only.
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 300 °C
30 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ASTM D1238
SABIC Innovative Plastics LNP LUBRICOMP LCL33EXQ PEEK
LNP* LUBRICOMP* LCL33EXQ is a compound based on Polyetheretherketone containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Easy Molding.
Melt Index of Compound 30 g/10 min

@Load 10.0 kg,
Temperature 345 °C
30 g/10 min

@Load 22.0 lb,
Temperature 653 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
Melt Index of Compound 30 g/10 min

@Load 10.0 kg,
Temperature 345 °C
30 g/10 min

@Load 22.0 lb,
Temperature 653 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics ULTEM SF2350 PEI Blend (Asia Pacific)
High flow Ultem blends for thin wall application
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 250 °C
30 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® SHF436HR PBT
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 250 °C
30 g/10 min

@Load 4.76 lb,
Temperature 482 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® SHF436HR PBT (Europe-Africa-Middle East)
PBT, Super High Flow, 30% glass reinforced,hydrolytically resistant.
Melt Index of Compound 30 g/10 min

@Load 10.0 kg,
Temperature 345 °C
30 g/10 min

@Load 22.0 lb,
Temperature 653 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific)
LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 265 °C
30 g/10 min

@Load 4.76 lb,
Temperature 509 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics Valox® V8280SF PBT+PET
High Modulus, PBT+PET, 40% Glass Reinforced, Mold Release, Super High Flow
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
A. Schulman PP 1901-01 Polypropylene High-Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1901-01 is a high-flow homopolymer polypropylene designed for the high-speed molding of thin walled, multi-cavity parts. ApplicationTypical applications of PP 1901-01 ar..
Melt Index of Compound 30 - 60 g/10 min
30 - 60 g/10 min
Zig Sheng Industrial ZISAMIDE® TP6603 Nylon 6
ZISAMIDE® TP6603 is a Polyamide 6. Application: compounding extrusionInformation provided by ZIG SHEN Industrial Co., LTD.
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® 8400 Polyolefin Elastomer
Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® 8401 Polyolefin Elastomer
Description: Engage® 8401 polyolefin elastomer is an ethyleneoctene copolymer that offers excellent performance in durable, flexible injection molded industrial and consumer goods. Engage® 8401 pr..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Dow Engage® 8407 Polyolefin Elastomer
Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p..
Melt Index of Compound 30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Polykemi AB POLYfill PP HBK1501515 Polypropylene, Multifiller High Gloss
Information provided by Polykemi AB
Melt Index of Compound 30 g/10 min

@Load 5.00 kg,
Temperature 300 °C
30 g/10 min

@Load 11.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FR9310 PPE (Europe-Africa-Middle East)
Noryl*FR9310 is a polyphenylene ether resin concentrate with nonhalogenated Flame retardant with Vicat of 165 deg C. Intended for use as an additive or a building block in a variety of thermoplasti..
Melt Index of Compound 30 g/10 min

@Load 10.0 kg,
Temperature 300 °C
30 g/10 min

@Load 22.0 lb,
Temperature 572 °F
MVR [cm^3/10 min]; ISO 1133
SABIC Innovative Plastics NORYL FE1630PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1630PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en..
Copyright © lookpolymers.com All Rights Reserved