Polymer Property : Flexural Modulus = 2.45 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.45 GPa
355 ksi
1.3 mm/min, 50 mm span; ASTM D790
Ovation Polymers OpteSTAT™ NC PP 0030 Polypropylene based Carbon Nanotube Compound
Material resistivity can be tailored to the application, while retaining the physical and thermal properties of the base polymer. Applications include components of disk drives, business machines or..
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East)
CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th..
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® DMX2415 PC (Asia Pacific)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Asia P..
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® DMX2415 PC (Europe-Africa-Middle East)
Lexan* DMX2415 is a polycarbonate resin with improved scratch resistance. Lexan* DMX2415 is available in transparent, translucent, and opaque colors.This data was supplied by SABIC-IP for the Europe..
Flexural Modulus 2.45 GPa
355 ksi
ISO 178
Radici Radilon® S35HR (dry) Nylon 6
Medium high viscosityInformation provided by Radici group.
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® LUX7430C PC COPOLYMER
Lexan* LUX7430C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® LUX7432C PC COPOLYMER (Asia Pacific)
Lexan* LUX7432C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Flexural Modulus 2.45 GPa
355 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® LUX7436C PC COPOLYMER
Lexan* LUX7436C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.2 mm / 5VA rating at 3.0mm a..
Flexural Modulus 2.45 GPa
355 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.45 GPa
355 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 2.45 GPa
<br>@Thickness 3.20 mm
356 ksi
<br>@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical XR409E ABS, Heat Resistance
Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch..
Flexural Modulus 2.45 GPa
355 ksi
ASTM D790
KYDEX® 110 Metallic Thermoplastic Fire-rated Sheet
Features:For deep or hard to form parts where good finished detail is requiredMore rigid than most thermoplastics, parts deform less when loadedMeets highest standard for chemical resistance for the..
Flexural Modulus 2.45 GPa
356 ksi
ASTM D790
Gromax CCP PBT 1100-104S
Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce..
Flexural Modulus 2.45 GPa
<br>@Thickness 3.20 mm
356 ksi
<br>@Thickness 0.126 in
15 mm/min; ASTM D790
LG Chemical XR407D ABS
Feature: Electric & Electronic HousingApplication: Electric & Electronic HousingCAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Chemical
Flexural Modulus 2.45 GPa
355 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific)
LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I..
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant
Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries.
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® BF-0677HF MABS, Unreinforced Scratch Resistant
Scratch resistant material that is used in TV housing and the exterior material for cleaner and air purifierInformation provided by Samsung Cheil Industries.
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Starex® LX-0989EXS ABS, Unreinforced Metallic-Look
Luminous Grade - gives aesthetics of a painted surface without painting. Reduces time, cost, and environmental hazards (such as soilvents).Information provided by Samsung Cheil Industries.
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose
Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries.
Flexural Modulus 2.45 GPa
356 ksi
ASTM D790
Samyang Trirex® 3025GRU10 Polycarbonate, 10% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
Flexural Modulus 2.45 GPa
355 ksi
15mm/min; ASTM D790
Denka MALECCA K-090 ABS
A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de..
Flexural Modulus 2.45 GPa
355 ksi
Tangent, chs 0.05 in/min; ASTM D790
Diamond Polymers ASA M-143
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Flexural Modulus 2.45 GPa
<br>@Thickness 3.17 mm
355 ksi
<br>@Thickness 0.125 in
ASTM D790
Calsak CS-72L General Purpose ABS Resin
Product Characteristics:High Impact, High GlossInjection molding grade
Flexural Modulus 2.45 GPa
355 ksi
ISO 178
Polyplastics Duracon® CP-15X Acetal Co-polymer (POM), Creep resistant, Creep resistant
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..