| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.15 g/cc | 1.15 g/cc | ASTM D 792 |
| Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0060 in/in @Thickness 0.126 in |
SABIC Method |
| Melt Flow | 38 g/10 min @Load 10.0 kg, Temperature 220 °C |
38 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D 1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 36.0 MPa | 5220 psi | Type I, 50 mm/min; ASTM D 638 |
| 38.0 MPa | 5510 psi | 50 mm/min; ISO 527 | |
| Tensile Strength, Yield | 50.0 MPa | 7250 psi | Type I, 50 mm/min; ASTM D 638 |
| 50.0 MPa | 7250 psi | 50 mm/min; ISO 527 | |
| Elongation at Break | 21 % | 21 % | Type I, 50 mm/min; ASTM D 638 |
| 25 % | 25 % | 50 mm/min; ISO 527 | |
| Elongation at Yield | 3.0 % | 3.0 % | Type I, 50 mm/min; ASTM D 638 |
| 3.0 % | 3.0 % | 50 mm/min; ISO 527 | |
| Tensile Modulus | 2.30 GPa | 334 ksi | 1 mm/min; ISO 527 |
| 2.47 GPa | 358 ksi | 50 mm/min; ASTM D 638 | |
| Flexural Yield Strength | 70.0 MPa | 10200 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| 70.0 MPa | 10200 psi | 2 mm/min; ISO 178 | |
| Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
| 2.41 GPa | 350 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.270 J/cm @Temperature -30.0 °C |
0.506 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
| 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 | |
| Izod Impact, Notched (ISO) | 3.00 kJ/m² @Temperature -30.0 °C |
1.43 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
| 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A | |
| Impact Test | 6.00 J @Temperature 23.0 °C |
4.43 ft-lb @Temperature 73.4 °F |
Instrumented Impact Total Energy; ASTM D 3763 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 81.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
45.0 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| CTE, linear, Transverse to Flow | 88.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
48.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 73.0 °C | 163 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 73.0 °C @Thickness 6.40 mm |
163 °F @Thickness 0.252 in |
unannealed; ASTM D 648 | |
| Vicat Softening Point | 78.0 °C | 172 °F | Rate B/50; ASTM D 1525 |
| 79.0 °C | 174 °F | Rate B/50; ISO 306 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Pencil Hardness test, 1kgf | F | ASTM D 3363 |