Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 78.0 °C | 172 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific) Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | 1000g; ASTM D-1525 |
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding
(discontinued **) Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be injection molded to produce pliable parts. It can also be used for making.. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | DIN 53460 |
Ineos Nova S-4600 High Impact Compact Polystyrene
(discontinued **) High impact polystyrene with excellent flow characteristics, a very high toughness and a high elongation. Main application are injection molding of technical parts and housings. For injection mold.. |
|||
Vicat Softening Point | 78.0 - 155 °C | 172 - 311 °F | Average value: 147 °C Grade Count:35 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Vicat Softening Point | 78.0 - 133 °C | 172 - 271 °F | Average value: 97.6 °C Grade Count:117 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | |
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of.. |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 211/W Rigid PVC, Antishock Extrusion Various antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RH 212/W Rigid PVC, Antishock Extrusion Outdoor antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free Small tubes for shoes |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 212/W Rigid PVC, Antishock Extrusion Lead Free Outdoor antishock profiles |
|||
Vicat Softening Point | 78.0 - 80.0 °C @Load 5.00 kg |
172 - 176 °F @Load 11.0 lb |
ISO R306 |
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock UV resistant |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
LyondellBasell Microthene® G MN70100 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and .. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m.. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a .. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
ICO Polymers ICOTEXâ„¢ 520-5050 500 Micron LDPE Powder Description: ICOTEX 520-5050 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and fa.. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ISO 306 |
Iran Petrochemical (PCC) HB5020 High Density Polyethylene HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
Lubrizol Estane® R175A Thermoplastic Polyurethane Type: Estane® R175A is a Shore 75A, plasticized grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Information Provided by The Lubrizol Corporation |
|||
Vicat Softening Point | 78.0 °C | 172 °F | |
Dow Primacor® 1420 Ethylene Acrylic Acid (EAA) Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | 50°C/hr; 50N |
Arkema Group Nakan® RMS 501 L PVC, Rigid Injection Molding Grade NAKAN RMS 501 L is a rigid polyvinyl chloride compound developed for injection molding of electrical boxes ( inside ).ISO data provided by the manufacturer, Arkema. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | 49 N; ISO 306 |
A.D. Compound Adene NTTAG Copolymer 40% Talc Filled Polypropylene Information provided by A.D. Compound |
|||
Vicat Softening Point | 78.0 °C | 172 °F | ASTM D1525 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Vicat Softening Point | 78.0 - 113 °C | 172 - 235 °F | Average value: 96.3 °C Grade Count:18 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Vicat Softening Point | 78.0 °C | 172 °F | A50; DIN 53460 |
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Vicat Softening Point | 78.0 - 159 °C | 172 - 318 °F | Average value: 141 °C Grade Count:18 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Vicat Softening Point | >= 78.0 °C | >= 172 °F | ASTM D 638 |
Karina 802-10/55-AY-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Vicat Softening Point | >= 78.0 °C | >= 172 °F | ASTM D 1525 |
Karina 802-10/93-AY-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |