Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Cycoloy® CY6010 PC+ABS
Cycoloy CY6010 resin is a flame retardant PC/ABS blend featuring excellent flow together with good impact and UL-94 V0 listing at 1.5mm. Its excellent flow combined with balanced heat and good pract..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® DMX9254 PC (Asia Pacific)
Lexan* DMX9254 resin is an injection moldable PC copolymer/ABS blend. This resin combines excellent scratch resistance with high flow and ductility. It contains non-brominated and non-chlorinated fl..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -40.0 °C
2.38 ft-lb/in²

@Temperature -40.0 °F
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® HTN 51G15HSL BK083 Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G15HSL BK083 is a 15% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East)
NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 1010A PEI (Asia Pacific)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 2200N PEI
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 2412EPR PEI
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Am..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl HF180 PPE+HIPS (Europe-Africa-Middle East)
NORYL HF180 is an unfilled, flame retardant material with a Vicat B/120 of 100°C according ISO 306. NORYL HF180 is V1 at 2.0 mm according UL94 and halogenThis data was supplied by SABIC-IP for th..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/A
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East)
Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
ISO 180/1A
Borealis Daplen™ EE340AE Polypropylene TPO Compound
Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80x10x4; ISO 180/1A
Eurostar Staramide ACF3 PA66, 15% Carbon Fiber Reinforced, Heat stabilized, Injection Molding
Staramide ACF3 is a 15% Carbon Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
80x10x4; ISO 180/1A
Eurostar Staramide BK8 PA6, 40% Mineral Fiber Filled, Injection Molded
Staramide BK8 is a 40% Mineral Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecoform® PO20 GR10 NL HS POM, 10% glass fiber reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecomid® NA40 GB30 NL HS PA6.6, 30% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA40 NL RM PA 6.6 low friction and wear
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecoform® PO30 GB20 NL HS POM, 20% glass bead reinforced, heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Eurotec® Tecomid® NA40 NL E PA6.6, unfilled, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural
Information provided by Eurotec®
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180
Ascend Performance Materials Vydyne® 21SPC1 Nylon 66, DAM
Vydyne® 21SPC1 is a general-purpose, improved-flow, lubricated PA66 resin available in natural color. 21SPC1 offers a balanced combination of properties characterized by high strength, rigidity, go..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® X6320 PBT+PC
X6320 is a mineral filled PBT/PC resin developed for automotive painted doorhandles. Key advantages are excellent surface finish, easy processing and paint quality.This data was supplied by SABIC-IP..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled
SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat..
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature -30.0 °C
2.38 ft-lb/in²

@Temperature -22.0 °F
ISO 180/1A
Sax Polymers SAXALEN PPH325GK20 Polypropylene Homopolymer, 20% Glass Filled
SAXALEN PPH325GK20 is a 10% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. It has a increased stiffness and a optimized warpage grade.Information ..