Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Polykemi AB POLYblend 85E PC/ABS-Blend
Information provided by Polykemi AB
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific)
Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties.
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics GELOY HRA170 ASA (Europe-Africa-Middle East)
GELOY HRA170 is a high heat resistant ASA+PC. It shows high impact retention, which can be positioned for various outdoor and indoor applications requiring superior heat aging properties and colour ..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics GELOY XP4025 ASA (Europe-Africa-Middle East)
GELOY XP4025 is a high heat modified ASA/PC blend, for automotive exterior applications. It shows very good properties, gloss and colour retention, as well as faster cycle time over competitive mate..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics Geloy XP4034 ASA (Europe-Africa-Middle East)
GELOY XP4034 is a high heat modified ASA+PC alloy. It is a weatherable, injection mouldable product which is available in a wide range of colours. The product is recommended for automotive unpainted..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Polikim KESTAMID® GRF Polyamide 6, Graphite Filled
Graphite and special lubricants are evenly dispersed in its entirety in this type of Polikim's cast polyamide. The material is dark grey colored. Kestamid®-GRF has a high degree of crystallinity an..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS
LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant.
Density 1.15 g/cc
0.0415 lb/in³
ASTM D 792
Shakespeare Isocorâ„¢ SC45BT Nylon 610
Isocorâ„¢ SC45BT is a medium viscosity PA-610 based copolymer. This resin is specifically suited for clear applications requiring increased solvent resistance and impact properties. Isocorâ„..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D 792
SABIC Innovative Plastics LNP Thermocomp MX88073 PP (Asia Pacific)
LNP* Thermocomp* MX88073 is a compound based on Polypropylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
SABIC Innovative Plastics NORYL LTA5020 PPE+PS
Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183-87
Wellman Wellamid® 22L-BL Engineering Grade Nylon 66
Description: Engineering Grade Nylon 66Information provided by Wellman.
Density 1.15 g/cc
0.0415 lb/in³
Dry Density
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH
Zellamid® 1100 is the registered trademark for Zell-Metall’s cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers ..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Unitika M2350 PA6, Dry
Nano composite nylonInformation provided by Unitika Ltd.
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Chengdu Polyster H4543 Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and injection grade. Contains improved color- stable antioxidants. Applications requiring high original color retention. Molded and injected products for consumer use, such as se..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Covestro Bayflex® 110-50 Polyurethane Elastomeric RIM, 15% Mineral Filled, MDI-based 2-Component Liquid System
Mineral filler is RRIMGLOS® 10013. 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialSc..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Cresset Powers Cress-Alon™ NF3040 4% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
Density 1.15 g/cc
0.0415 lb/in³
JIS-Z-8807
Denka REOMER G G8355 Thermoplastic Elastomer, For Injection Molding
Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive..
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, 15% Milled Glass Filled, MDI-based 2-Component Liquid System
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
EMS-Grivory Grivory® TR XE 4139 black 9231 PA*
Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a..
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
Eurotec® Tecomid® NT40 NL MB PPA, impact modified, heat stabilized, natural
Information provided by Eurotec®
Density 1.15 g/cc
0.0415 lb/in³
Silicone Property; Arlon SQA-TMS-024
Arlon R37230R006 0.006" (0.152 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate
Design/Construction: Liner: FEP Add-on: Uncured Silicone Rubber Substrate: PTFE Coated Fiberglass This data represents typical values for the production material. The data should not be used to wri..
Density 1.15 g/cc
0.0415 lb/in³
A. Schulman ComAlloy Hiloy® 261 Glass Reinforced, Modified SMA
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Density 1.15 g/cc
0.0415 lb/in³
ISO 1183
DSM Arnitel® EB464-01 TPC-ET
Antisqueak Blow Molding Grade
Density 1.15 g/cc
0.0415 lb/in³
(DAM)
Ineos ABS Triax® DP 3155 ABS + Polyamide Blend (Conditioned)  (discontinued **)
Key Features:Contains FillerSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS..
Density 1.15 g/cc
0.0415 lb/in³
GB1033
Beijing Evergrow Resources MC Nylon
Information provided by Beijing Evergrow Resources.
Density 1.15 - 1.18 g/cc
0.0415 - 0.0426 lb/in³
Average value: 1.16 g/cc Grade Count:6
Overview of materials for Acrylic, Impact Modified Sheet
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified Sheet". Each property range of values reported is minimum and maximum values of..
Density 1.15 g/cc
0.0415 lb/in³
Arkema Group Oroglas® SG 10 Acrylic, Gamma Radiation Resistant  (discontinued **)
OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no advers..