Polymer Property : Vicat Softening Point = 172 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 78.0 °C

@Load 1.00 kg
172 °F

@Load 2.20 lb
ISO 306/A
Polimeri Europa Greenflex® ML 21 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed.Main Applic..
Vicat Softening Point 78.0 °C
172 °F
Rate B/50; ASTM D 1525
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific)
Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region.
Vicat Softening Point 78.0 °C
172 °F
1000g; ASTM D-1525
ExxonMobil Optema® TC-020 Ethylene Methyl Acrylate for Injection Molding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.6.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be injection molded to produce pliable parts. It can also be used for making..
Vicat Softening Point 78.0 °C
172 °F
Eastman Tenite 130-33 Cellulose Acetate  (discontinued **)
33% Plasticized, contains 100% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
Vicat Softening Point 78.0 °C
172 °F
LyondellBasell Lupolen® 5261 ZS HDPE, Blow Molding Grade
Relatively high viscosity blow molding grade (similar to Lupolen 5261 Z), but more resistant to stress cracking) for rigid, stackable and highly shock resistant containers for packaging all types of..
Vicat Softening Point 78.0 - 80.0 °C

@Load 5.00 kg
172 - 176 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RH 211/W Rigid PVC, Antishock Extrusion
Various antishock profiles
Vicat Softening Point 78.0 - 80.0 °C

@Load 5.00 kg
172 - 176 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RK 115 Rigid PVC, Extrusion Lead Free
Small tubes for shoes
Vicat Softening Point 78.0 - 80.0 °C

@Load 5.00 kg
172 - 176 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RKS 315/W Rigid PVC, Antishock Extrusion Lead Free
Various profiles antishock
Vicat Softening Point 78.0 - 80.0 °C

@Load 5.00 kg
172 - 176 °F

@Load 11.0 lb
ISO R306
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free
Various profiles, antishock UV resistant
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
LyondellBasell Microthene® G MN71400 Low Density Polyethylene
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
Vicat Softening Point 78.0 °C
172 °F
A; ISO 306
FKuR Kunststoff Bio-Flex® F 2110 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
ICO Polymers ICOFLOâ„¢ 510-5049 400 Micron LDPE Powder
Description: ICOFLO 510-5049 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
ICO Polymers ICOFLOâ„¢ 510-5050 500 Micron LDPE Powder
Description: ICOFLO 510-5050 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma..
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
ICO Polymers ICOFLOâ„¢ 510-5052 1200 Micron LDPE Powder
Description: ICOFLO 510-5052 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in m..
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
ICO Polymers ICOTEXâ„¢ 520-5016 300 Micron LDPE Powder
Description: ICOTEX 520-5016 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Key Characteristics: good melt flow and a ..
Vicat Softening Point 78.0 °C
172 °F
ISO 306
Iran Petrochemical (PCC) HB5020 High Density Polyethylene
HB-5020 is a high molecular weight high density polyethylene.Applications: extrusion blow moldingInformation provided by Iran Petrochemical Commercial Co.
Vicat Softening Point 77.8 °C
172 °F
ASTM D1525
Teknor Apex Sinvicomp SBC 3707 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi..
Vicat Softening Point 77.8 °C
172 °F
ASTM D1525
Teknor Apex Sinvicomp SBF 3748 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex
Vicat Softening Point 77.8 °C
172 °F
ASTM D1525
Teknor Apex Sinvicomp SIC 3710 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: High Impact ResistanceUses: Rigid Packing; Tubing Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
Lubrizol Estane® R175A Thermoplastic Polyurethane
Type: Estane® R175A is a Shore 75A, plasticized grade thermoplastic polyurethane (TPU).Uses: Injection Molding.Information Provided by The Lubrizol Corporation
Vicat Softening Point 78.0 °C
172 °F
ASTM D1525
UBE J5019 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Vicat Softening Point 78.0 °C
172 °F
5kg load; ISO 306
Eastman Spectar® 14471 Copolyester
Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use ..
Vicat Softening Point 78.0 °C
172 °F
Dow Primacor® 1430 Ethylene Acrylic Acid (EAA)
Film properties below based on a film thickness of 60 µm. Data provided by Dow Chemical.
Vicat Softening Point 78.0 °C
172 °F
50°C/hr; 50N
Arkema Group Nakan® RMS 501 L PVC, Rigid Injection Molding Grade
NAKAN RMS 501 L is a rigid polyvinyl chloride compound developed for injection molding of electrical boxes ( inside ).ISO data provided by the manufacturer, Arkema.
Vicat Softening Point 77.8 °C
172 °F
ASTM D1525
Alliance Polymers Zythane™ 5060A Thermoplastic Polyurethane Elastomer
Zythane™ 5060A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Vicat Softening Point 78.0 °C
172 °F
49 N; ISO 306
A.D. Compound Adene NCTAG Copolymer 50% CaCO3 Filled Polypropylene
Information provided by A.D. Compound
Vicat Softening Point 78.0 - 113 °C
172 - 235 °F
Average value: 96.3 °C Grade Count:18
Overview of materials for Cellulose Acetate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr..
Vicat Softening Point 78.0 °C
172 °F
A50; DIN 53460
Lubrizol ESTANE® 58437 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Vicat Softening Point 77.8 °C
172 °F
ASTM D1525
Teknor Apex Sinvicomp SBB 3710 Polyvinyl Chloride, Rigid
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; High Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provide..