| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycolac® S703T ABS (Europe-Africa-Middle East)
CYCOLAC S703T is a super high flow ABS developed for thin wall injection/compression moulding applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer
Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*3; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® HPB3144G PC Copolymer
Standard flow, transparent, high purity polycarbonate copolymer resin with reduced oxygen permeability and water vapor transmission rate. For medical devices and pharmaceutical applications. Health..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -40.0 °C
|
2.38
ft-lb/in² <br>@Temperature -40.0 °F
|
ISO 180/1A |
|
DuPont Performance Polymers Rynite® FR515 BK507 PET
(Unverified Data**)
Rynite® FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8mm(0.03in). Has a 140C temp index. Excellent balance of electr..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer
EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
DAM; ISO 180/1A |
|
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**)
Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1010RF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact Compliant in recognized colors.This data was supplied by SABIC-IP for the Americas reg..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1010RV PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 1010X PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized color..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem 2412EPR PEI (Europe-Africa-Middle East)
40% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem AUT230M PEI
Transparent polyetherimide (Tg 247 degC). Contains low level of mold release. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are ..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem HATX200 PEI+PCE (Europe-Africa-Middle East)
High flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compli..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East)
Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Valox® VX8015U PBT+PET (Europe-Africa-Middle East)
VALOX VX8015U is a UV stabilized, 15% glass reinforced PBT+PET injection moulding resin with improved surface finish quality characteristics versus VALOX 815. This grade is 815 with improved gloss a..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/A |
|
Styrolution Terluran® HH-112 Q109 ABS
Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/A |
|
Styrolution Terblend® N 3154 ASA / PA, 8% Mineral filled
Terblend N 3154 is an 8% mineral filled ABS/PA blend with good dimensional stability and enhanced rigidity.High dimensional stabilityEnhanced rigidityMineral filled (8%)Information provided by Styro..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Noryl EN110 PPE+HIPS (Europe-Africa-Middle East)
NORYL EN110 is an extrusion material with a Vicat B/120 of 115°C according ISO 306. NORYL EN110 is a standard extrusion grade for applications where medium temperature resistance is required.This..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Domo 2448L Polypropylene Copolymer
Information provided by Domo.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 0.000 °C
|
2.38
ft-lb/in² <br>@Temperature 32.0 °F
|
ISO 180/1A |
|
Domo 2600PC Polypropylene Copolymer
Information provided by Domo.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
80x10x4; ISO 180/1A |
|
Eurostar Staramide B28N PA6, Nucleated, Injection Molded
Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NA30 NL RM PA6.6, MoS2 modified, natural
Information provided by Eurotec®
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Eurotec® Tecomid® NB40 NL XA 20 PA 6 unreinforced, UL94 V0
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/1A |
|
Eurotec® Tecodur® PB70 GR10 NL PBT 10% glass fiber reinforced
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180/A |
|
BASF Ultraform W 2320 003 UNC Q600 POM
Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains ..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
ISO 180 |
|
Ascend Performance Materials Vydyne® 20NSP1 Nylon 66, Conditioned
Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 43% Filler by Weight Additive:Nucleating AgentLubricant Features:Fast Molding CycleGeneral PurposeGood Mold Release Good..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature 23.0 °C
|
2.38
ft-lb/in² <br>@Temperature 73.4 °F
|
ISO 180/1A |
|
Sax Polymers SAXALEN PPC339T20 Polypropylene Copolymer, 20% Talc Filled
SAXALEN PPC339T20 is a 20% mineral filled Polypropylene - Copolymer intended for injection molding with good flow properties und higher stiffness. The PP-Copolymer has low warpage behaviors and good..
|
|||
| Izod Impact, Notched (ISO) |
5.00
kJ/m² <br>@Temperature -30.0 °C
|
2.38
ft-lb/in² <br>@Temperature -22.0 °F
|
80*10*4; ISO 180/1A |
|
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East)
GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East ..
|
|||