Polymer Property : Flexural Modulus = 2.41 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.41 GPa
350 ksi
Tangent; ASTM D790
RheTech Products T20P100-00UV 20% Talc Reinforced Polypropylene, UV Stabilized, Natural
Applications: Electronic housingsConsolesIP componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.41 GPa
350 ksi
Tangent; ASTM D790
RheTech Products T20P104-01 20% Talc Reinforced Polypropylene, Black
Applications: Electronic housingsIP componentsHVAC ducts - air distributionClose out panelDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 2.41 GPa
350 ksi
Test Method I, Procedure B (chs speed 0.05 in/min), Tangent; ASTM D790
Network Polymers NPP 30-2000 TF33
Description: 33% Talc Filled Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Polymer Resources PPX-FR3 Modified-PPO, V-1 Flame Retardant
Modified-Polyphenylene Oxide, V-1 Flame Retardant, 265F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Polymer Resources PPX-SF2 Modified-PPO, Structural Foam Grade, Flame Retardant
Modified-Polyphenylene Oxide, Structural Foam Grade, Standard FlowFeatures: • Flame Retardant • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mec..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy
Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Ravago Manufacturing Americas Hylac® GP55 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Modulus 2.41 GPa
350 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® LUX9130T PC COPOLYMER (Asia Pacific)
LUX9130T Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm / 5VA rating at 6.0mm and is U..
Flexural Modulus 2.41 GPa
350 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS
Color package may affect performance. Visual Fx PC+ABS in various metallic (sparkle) colors. High heat/good flow characteristics. Appliance/automotive/telecommunication uses.
Flexural Modulus 2.41 GPa

@Thickness 3.17 mm
350 ksi

@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-10R-CL(V) 10 MFI UV Stabilized Clear Polycarbonate with Release
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
PolyOne Lubri-Tech™ ATH-000/20T Homopolymer Acetal - 20% PTFE Lubricated  (discontinued **)
Data provided by PolyOne.
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
LG Chemical Lupoy 1201-15 Polycarbonate Resin
Description: LUPOY PC 1201-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength...
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
LG Chemical Lupoy 1301EP30 Polycarbonate Resin
Description: LUPOY PC 1301EP-30 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
LG Chemical Lupoy 1200HP-15 Polycarbonate Resin
Description: LUPOY PC 1200HP-15 resin is designed for extrusion and injection molding products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strengt..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
LG Chemical Lupoy 1302HP-10 Polycarbonate Resin
Description: LUPOY PC 1302HP-10 resin is designed for extrusion products. It exhibits an excellent physical property balance of heat resistance, transparency and impact strength.Main Characteristics..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
LG Chemical Lupoy 1303AH-15 Polycarbonate Resin
Description: LUPOY PC 1303AH-15 Tint Polycarbonate Resin is designed for injection molding of auto-headlamps. It exhibits an excellent physical property balance of heat resistance, transparency and ..
Flexural Modulus 2.41 GPa
350 ksi
secant; ASTM D790
Spartech PP5140 Talc Filled Homopolymer
Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Techmer ES HiFill® PBT E
Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Extrusion and Injection MoldingInformation provided by TP Composites, Inc.
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Techmer ES Plastiblend® ABS LG UV
Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc.
Flexural Modulus 2.41 GPa
350 ksi
Method I (3 point load), 2.0 mm/min; ISO 178; ASTM D790
Styron CALIBREâ„¢ 200-3 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-3 polycarbonate resin is produced in compliance with the US Food and Drugs Administration (FDA) and EU food contact regulation. This resin provides excellent impact resis..
Flexural Modulus 2.41 GPa
350 ksi
Method I (3 point load), 2.0 mm/min; ASTM D790
Styron CALIBREâ„¢ 200-6 Polycarbonate Resin
Overview: CALIBREâ„¢ 200-6 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistance..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Styron CALIBREâ„¢ 201-22 Polycarbonate
Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010.
Flexural Modulus 2.41 GPa
350 ksi
3-points, 2 mm/min; ASTM D790
Styron CALIBREâ„¢ 2061-22 Polycarbonate
CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and..
Flexural Modulus 2.41 GPa
350 ksi
0.125 in, injection molded, unannealed; ASTM D790
Styron EMERGEâ„¢ 4530-15 Polycarbonate
EMERGEâ„¢ PC 4530-15 advanced resin is a general purpose polycarbonate resin offering ultraviolet light stability, ignition resistance, heat resistance and excellent toughness. Applications: Co..
Flexural Modulus 2.41 GPa
350 ksi
Tangent; ASTM D790
Plastics Group Polifil® RMC-40 40% Calcium Carbonate-Reinforced Polypropylene, High Impact
Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Formosa Plastics Formolon® AWS Compound
AWS Powder Profiler Compound Series The AWS compounds have been designed for profile extrusion in indoor and non-weatherable applications and substrates for outdoor applications. They exhibit a natu..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Ensinger Tecast Vekton™ 6PA Blue Unfilled Cast Nylon 6 (PA6)
Tecast 6PA Blue is a blue cast nylon with properties similar to natural nylon 6.General Tecast Cast Nylon Information: Tecast cast nylon, available in a variety of grades, offers a combination of go..
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Ensinger Tecast Vekton™ 6PAL Oil-Filled Cast Nylon 6 (PA6)
Tecast® 6PAL is used in applications requiring excellent bearing and wear properties where external lubrication is difficult or impractical.General Tecast® Cast Nylon Information: Tecast cast nylo..
Flexural Modulus 2.41 GPa
350 ksi
Tangent; ASTM D790
RheTech Products HP506-01B 22% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black
Applications: Underhood componentsLamp housingsHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products.