Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
Manufacturer | Polykemi AB |
Trade Name | POLYblend |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Polykemi AB POLYblend 83FR PC/ABS-Blend, Flame Retardant, Halogen Free.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.19 g/cc | 0.0430 lb/in³ | ISO 1183 |
Linear Mold Shrinkage | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | With Flow; ISO 2577 |
0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | Across Flow; ISO 2577 | |
Melt Index of Compound | 35 g/10 min @Load 5.00 kg, Temperature 260 °C |
35 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Elongation at Yield | 5.5 % | 5.5 % | ISO/R527 |
Flexural Strength | <= 95.0 MPa | <= 13800 psi | ISO 178 |
Flexural Modulus | 2.30 GPa @Temperature 23.0 °C |
334 ksi @Temperature 73.4 °F |
ISO 178 |
Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
Deflection Temperature at 1.8 MPa (264 psi) | 95.0 °C | 203 °F | 120°C/h; ISO 75/1 |
Vicat Softening Point | 105 °C @Load 5.001 kg |
221 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Flammability, UL94 | V-0 @Thickness 1.60 mm |
V-0 @Thickness 0.0630 in |
|
Glow Wire Test | 960 °C @Thickness 1.60 mm |
1760 °F @Thickness 0.0630 in |
IEC 695-2-1 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
Mold Temperature | 70.0 - 100 °C | 158 - 212 °F | |
Drying Temperature | 80.0 - 100 °C | 176 - 212 °F | |
Dry Time | 2 - 8 hour | 2 - 8 hour | in circulation dryer |
2 - 8 hour | 2 - 8 hour | in fresh-air dryer | |
2 - 8 hour | 2 - 8 hour | in desiccant air dryer | |
Injection Pressure | 90.0 - 150 MPa | 13100 - 21800 psi | |
Back Pressure | 0.500 - 1.50 MPa | 72.5 - 218 psi |
Descriptive Properties | Value | Comments |
---|---|---|
Holding Pressure () | 20-50 | % of injection pressure |
Injection Speed () | High |