| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Polykemi AB POLYblend 85VB PC/ABS-Blend, Flame Retardant
Information provided by Polykemi AB
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Do not melt above 300°C |
|
Nilit Nilamid B3N Unfilled, Nucleated PA6
Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
DuPont Performance Polymers Crastin® LW9030FR BK851 PBT
(Unverified Data**)
Crastin® LW9030FR BK851 is a 30% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
DuPont Performance Polymers Crastin® S600F40 BK851 PBT
(Unverified Data**)
Crastin® S600F40 BK851 is an unreinforced, lubricated, low viscosity, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Plastcom SLOVAMID 6 GF 10 FRG 5 Polyamide 6, 10% Glass Fiber, Flame Retardant
FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fiber. Application: impacted mouldings with high strength applied in automotive, electrical, engineering and consumer-goo..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength
FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme..
|
|||
| Melt Temperature | 240 - 250 °C | 464 - 482 °F | Extrusion |
|
DuPont Performance Polymers Hytrel® 6646 NC010 TPC-ET
(Unverified Data**)
Hytrel® 6646 NC010 is a medium modulus grade with nominal hardness of 66D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like ..
|
|||
| Melt Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
|
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET
(Unverified Data**)
Hytrel® DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 49D and contains fine particle size carbon black.In..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | Start Point: 250°C |
|
Kingfa LONOY 1200 PC/PBT Alloy
Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 250°C |
|
Kingfa PBT-RG152 Flame Retardant, 15% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | Start Point: 250°C |
|
Kingfa PC-S609 Toughened PC
Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
LG Chemical LUPOS HR-2407 Heat Resistant SAN, 40% Glass Fiber Reinforced
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
LATI Latiohm 62-08 PD02 G/30 PPA, 30% Glass Fiber Reinforced
Dissipative product based on Polyamide 6 (PA6). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
Lubrizol Isoplast® 101LGF40BLK Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
|
|||
| Melt Temperature | 240 - 275 °C | 464 - 527 °F | |
|
A. Schulman SCHULAMID® 6 NV12 Easy Flow Low Viscosity Nylon 6
Information provided by A. Schulman.
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection Molding; ISO 294 |
|
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradegeneral purposecompared to FR 3000 improved chemical resistance and stress cracking behaviorVicat/B 120 temperature = 97 °CUL 94 V-0 at 1.5 mmPreprocessingMax. Water content
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Covestro Bayblend® FR 3002 Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradefor notebooks and thinwall applicationsVicat/B 120 temperature = 99 °CUL-listing 94 V-0 (1.2 mm)antimony- chlorine- and bromine-free flame retardantglow wire test (GWFI): 960..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Covestro Bayblend® FR 3005 HF Polycarbonate + ABS, Flame Retardant Grade
Injection molding gradevery easy-flow gradeVicat/B 120 temperature = 96 °CUL-listing 94 V-0 (1.5 mm) antimony-, chlorine- and bromine-free flame retardantPreprocessingMax. Water content
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection molding; ISO 294 |
|
Covestro Bayblend® FR3000 BBS081 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Impro..
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
Covestro Bayblend® W85 XF* Polycarbonate + ASA
Developmental product(PC+ASA) blendinjection molding grade with improved weather resistanceoptimized heat ageing stabilityhigh heat resistanceVicat/B 120 = 132 °CPreprocessingMax. Water content
|
|||
| Melt Temperature | 240 °C | 464 °F | DAM; optimum; Extrusion |
|
DuPont Performance Polymers Zytel® ST811HS BK038 Nylon 6
(Unverified Data**)
Zytel® ST811HS BK038 is a flexible, non-plasticized, black Super Tough nylon 6 resin developed for extrusion and injection molding applications such as cable and rope jacketing, hose inner cores an..
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG10HU PA6, 50% Glass Fiber Filled, UV and Heat Stabilized, Injection Molded
Staramide BG10HU is an UV and Heat Stabilized, 50% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded
BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Melt Temperature | 240 - 270 °C | 464 - 518 °F | |
|
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded
Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Melt Temperature | 240 - 280 °C | 464 - 536 °F | |
|
E-Polymers TEKALOY® G70NHT Non Halogen Flame Retardant Impact Resistance PC/ABS Alloy
PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan..
|
|||
| Melt Temperature | 240 °C | 464 °F | Injection molding; ISO 294 |
|
Covestro Bayblend® FR630 GR PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
|
|||
| Melt Temperature | 240 - 285 °C | 464 - 545 °F | |
|
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
|
|||
| Melt Temperature | 240 °C | 464 °F | Optimal |
|
BASF Ultramid® Seal-Fit PA6/66 (Dry)
Description: Transparent, tough, amorphous copolyamide for injection molding, specially developed for tight overmoulding of metal inlays.Information provided by BASF
|
|||
| Melt Temperature | 240 - 260 °C | 464 - 500 °F | |
|
Eurostar Star L PA6 D83 PA6, Injection Molded
Star L PA6 D83 is a PTFE/Proprietary Additive Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||