| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Vicat Softening Point | 105 °C | 221 °F | |
| Plastcom SLOVALEN PC 79 T 20 PP/C reinforced with 20% mineral filler Features: Modified PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal. Decreased shrinkage. Antistatic agent. Delivered in natural mode and i.. |
|||
| Vicat Softening Point | 105 °C @Load 1.00 kg |
221 °F @Load 2.20 lb |
ISO 306/A |
| Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics Cycolac® INP572 ABS High molecular weight SAN, functions as a carrier resin for color concentrates. Can be used as compounding additives for polymer blends. Can be blended with high rubber graft modifier resins to pro.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics Cycoloy® EFX830ME PC Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering metallic / sparkle look with minimal flow line visibilityThis data was supplied by SABIC-.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
| SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
| Vicat Softening Point | 105 °C | 221 °F | ASTM D1525 |
| Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
| SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
| SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
| Vicat Softening Point | 105 °C | 221 °F | ASTM D1525 |
| ExxonMobil LD 117.03 Blown Overwrap Film Resin
(discontinued **) LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma.. |
|||
| Vicat Softening Point | 105 °C @Load 5.00 kg |
221 °F @Load 11.0 lb |
50°C/h; ASTM D1525 |
| LG Chemical LI942 Heat Resistant ASA Description: High Heat ASAApplication: Automotive Part (Roof Rack Cover)CAS: 26299-47-8Information provided by LG Chemical |
|||
| Vicat Softening Point | >= 105 °C | >= 221 °F | ISO 306A |
| Lucite International Perspexâ„¢ XT IM50 Acrylic Extruded Sheet PERSPEX extruded sheet has a lower molecular weight making it easy to vacuum form and the extrusion process gives excellent thickness tolerance and is economical for long production runs.Information.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ISO 306 |
| SABIC Innovative Plastics NORYL SE90 PPE+HIPS (Europe-Africa-Middle East) NORYL SE90 is an unfilled, flame retardant material with a Vicat B/120 of 110°C according ISO 306. NORYL SE90 is V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
| Vicat Softening Point | 105 °C | 221 °F | VST/A/50; ISO 306 |
| Styrolution Luran® S 757 G UV White 37019 ASA Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | VST/A/50; ISO 306 |
| Styrolution Luran® S 777 K UV Black 56625 ASA Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
| Vicat Softening Point | 105 °C | 221 °F | B/120; ISO R306 |
| Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
| Vicat Softening Point | 105 °C | 221 °F | (50 °C/h / 50N) - B/50; ISO 306 |
| Styrolution Terblend® N NMX04 ABS/PA6 (Dry) Terblend N NMX04 is an ABS/PA6 blend specially developed for painted exterior applications, combining impact resistance with excellent processability and paintability.Information provided by STYROLU.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/50; ASTM D1525 |
| SABIC Innovative Plastics Valox® V3900WX PBT+PC (Asia Pacific) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
| Vicat Softening Point | 105 °C | 221 °F | 10 N; ISO 306 |
| Borealis Steripeel™ WE150CF PO Compound for Sterilizable Peelable Film Applications Steripeel WE150CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WE150CF is suitable for.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | 10 N; ISO 306 |
| Borealis Borpeel™ WD255CF PO Compound for Non Sterilizable Peelable Film Applications Borpeel WD255CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Borpeel WD255CF is suitable for vari.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | 50°C/h 50N; ISO 306 |
| DSM Arnitel® PB582-H 58 Shore D, Blow Molding Grade, Heat Stabilized Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | 0.125 inch, 1 Kg; ASTM D1525 |
| Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
| Vicat Softening Point | 105 °C @Load 1.00 kg, Thickness 3.17 mm |
221 °F @Load 2.20 lb, Thickness 0.125 in |
ASTM D1527 |
| Diamond Polymers DIAMALOY ABSPC 750 HF ABS/PC Alloy, Non-Halogen, Flame Retardant Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
| Vicat Softening Point | 105 °C | 221 °F | ASTM D1525 |
| Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
| Vicat Softening Point | 105 °C | 221 °F | |
| BASF Procom® D 1012 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
| Vicat Softening Point | 105 °C | 221 °F | 120°C/hr, 1 kg; ASTM D1525-B |
| Americas Styrenics STYRON™ 668 General Purpose Polystyrene Resin STYRON™ 668 is a general purpose polystyrene with medium flow and a balance of heat resistance and stiffness characteristics that make it suitable for applications such as CD jewel boxes. STYRON™.. |
|||
| Vicat Softening Point | 105 - 118 °C | 221 - 244 °F | Average value: 113 °C Grade Count:8 |
| Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
| Vicat Softening Point | 105 °C | 221 °F | Rate B/120; ISO 306 |
| SABIC Innovative Plastics GELOY CR7500 ASA High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||