Polymer Property : Back Pressure = 72.5 psi Product List

Processing Properties

Tips: 30 items are displayed at most.
Processing Properties Metric English Comments
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Polykemi AB POLYblend 85E PC/ABS-Blend
Information provided by Polykemi AB
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Polykemi AB POLYfill PP CIP15015 UV Polypropylene, Mineral Reinforced
Information provided by Polykemi AB
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Polykemi AB POLYfill PP EIP16020 F PP Mineral Reinforced, Extrusion Grade, Low CLTE
Information provided by Polykemi AB
Back Pressure 0.500 - 2.00 MPa
72.5 - 290 psi
Injection molding
Hexion Bakelite™ EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage  (dis
Epoxy molding compound, inorganically filled, glass fiber reinforced, highly heat resistant, good electrical even at higher temperatures, very slight post shrinkage, increased media resistance, UL l..
Back Pressure 0.500 - 2.00 MPa
72.5 - 290 psi
Injection molding
Hexion Bakelite™ PF 85 Phenolic Formaldehyde Resin, UL Listed  (discontinued **)
Phenolic molding compound, organically filled, reinforced with cotton fibers, average notched impact strength, UL listed molding compound 1.5 mm/HB (BK, BN).Application areas: Switch covers, rolls, ..
Back Pressure 0.500 - 2.00 MPa
72.5 - 290 psi
Injection molding
Hexion Bakelite™ PF 6507 Phenolic Formaldehyde Resin, Elasticized, Low Shrinkage, Resistant to High Temperatures, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, elastomer modified, galvanizable, heat resistant, good media resistance, high dimensional stability at raised temperature, hi..
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Stellarchem GP-975 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Stellarchem LP-880 TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Stellarchem MP-835B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection Molding
Stellarchem MP-845B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Akro-Plastic Akroloy® PA GF 60 (2844) PA 6.6 & PA6I/6T Dry, 60% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G80A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer
Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.500 - 1.00 MPa
72.5 - 145 psi
Injection
Alliance Polymers Zythane™ 6075A Thermoplastic Polyurethane Elastomer
Zythane™ 6075A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Back Pressure 0.500 - 0.848 MPa
72.5 - 123 psi
Injection
Alliance Polymers Viprene™ P70A-22U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ P70A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Back Pressure 0.500 - 2.00 MPa
72.5 - 290 psi
Injection molding
Hexion Bakelite™ PF 4041 Phenolic Formaldehyde Resin, Resistant to High Temperatures  (discontinued **)
Phenolic molding compound, glass fiber reinforced and inorganically filled, elasticized. Very good heat resistance, very good mechanical properties, reduced mold shrinkage and post-shrinkage, good ..
Back Pressure 0.500 - 2.00 MPa
72.5 - 290 psi
Injection molding
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
Back Pressure 0.500 - 15.0 MPa
72.5 - 2180 psi
Injection Molding
LG Chemical LUTENE-H ME8000 HDPE
Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated..