| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | DIN 53453; ASTM D256 |
| Kolon KOPA® KN133G50 G/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
| Izod Impact, Notched | >= 1.77 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 3.31 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
| LG Chemical LUPOL HM5302W PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 26221-73-8 and 14807-96-6Information provided by LG Chemical |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® CR-0760 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced WNP GradeInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SR-0310FM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® CR-0760 ABS, Unreinforced Good chemical resistanceInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SD-0150W ABS, Unreinforced WNP GradeInformation provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SR-0310FM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm @Thickness 6.35 mm |
3.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
| Samsung Cheil Industries Starex® SR-0320BM ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | ASTM D256 |
| PlastxWorld Veroplas PB3400 Nylon 66 general purpose, 40% glass filled injection molding gradeInformation provided by PlastxWorld Inc. |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | |
| Zylog Hipolyene® 3080 HC RM Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | |
| Zylog Hipolyene® 3152 MC Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | |
| Zylog Hipolyene® 1532 HC EX Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | ASTM D256 |
| E-Polymers TEKAPPO® JF6 Un-Reinforced Flame Retardant Heat Resistance M-PPO Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a.. |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | ASTM D256 |
| Cheng Yu Plastic E500 PC/PET |
|||
| Izod Impact, Notched | 1.77 J/cm | 3.31 ft-lb/in | ASTM D256 |
| E-Polymers TEKAMID® JN1 PPE+PA66 Un-reinforced High flow Heat resistance PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||