Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.011 - 0.020 cm/cm | 0.011 - 0.020 in/in | ASTM D955 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.020 cm/cm | 0.014 - 0.020 in/in | ASTM D955 |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | ASTM D955 |
PolyOne Elastamax™ HTE 1102 Styrene Butadiene Block Copolymer (SBC) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
LG Chemical LUCEL HI525L POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm | 0.018 - 0.020 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RX93237 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RX93237 is a compound based on Nylon 66 resin containing PTFE, Silicone, MOS2. |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.014 - 0.020 cm/cm @Thickness 3.20 mm |
0.014 - 0.020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Xenoy® 6620 PBT+PC (Asia Pacific) Impact modified, highly chemical resistant polyester/polycarbonate alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp FF008L PE LNP* Thermocomp* FF008L is a compounding based on Polyethylene containing glass fiber. Added characteristics include Low Extractible.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.012 - 0.020 cm/cm | 0.012 - 0.020 in/in | on tensile bar; SABIC Method |
SABIC Innovative Plastics Noryl GTX VP7133 PPE+PA (Europe-Africa-Middle East) Noryl GTX VP7133 is an unfilled extrusion grade which offers high heat resistance in combination with high meltstrength.The material is especially designed for thermal break profiles which are used .. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Lubricomp LL003E PEEK LNP* Lubricomp* LL003E is a compound based on Polyetheretherketone (PEEK) containing PTFE. Characteristics of this grade are: Easy Molding and Internally Lubricated.This data was supplied by SABIC.. |
|||
Linear Mold Shrinkage, Flow | 0.0090 - 0.020 cm/cm @Time 86400 sec |
0.0090 - 0.020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | DIS 294-4 |
Wellman Wellamid® MRT1487 BK Nylon 66, 32% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | on Tensile Bar; E2P method |
Eurostar Staramide A28 PA66, Injection Molding Staramide A28 is an Unreinforced, Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.018 - 0.020 cm/cm @Thickness 4.00 mm |
0.018 - 0.020 in/in @Thickness 0.157 in |
E2P method |
Eurostar Starpylen HU 30E4 ECR PP, Mineral Filled, Injection Molding Starpylen HU 30E4 ECR is a reinforced Polypropylene with a low carbon footprint renewable mineral filler, Injection Molding Resin (also known as HUS30E4ECR)Information provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ASTM D955 |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Linear Mold Shrinkage, Flow | 0.010 - 0.020 cm/cm | 0.010 - 0.020 in/in | ASTM D955 |
Elastocon TPE Technologies Elastocon® 8088BL Thermoplastic Elastomer Elastocon® 8088BL is a black lubricated thermoplastic elastomer formulated for applications that require high impact resistance and a reduced coefficient of friction. Elastocon® 8088BL is well sui.. |
|||
Linear Mold Shrinkage, Flow | 0.015 - 0.020 cm/cm | 0.015 - 0.020 in/in | |
Solvay TECHNYL® 2210HS PA66, DRY Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe.. |
|||
Linear Mold Shrinkage, Flow | 0.016 - 0.020 cm/cm | 0.016 - 0.020 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |