| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.017 - 0.021 cm/cm | 0.017 - 0.021 in/in | ASTM D955 |
| PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm | 0.017 - 0.023 in/in | ASTM D955 |
| PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE) Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
| Network Polymers Softflex® 5300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
ISO 294-4 |
| DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
| Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standar.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
| LG Chemical LUCEL HI515W POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: Gears, Automobile ClipCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
ASTM D955 |
| LG Chemical LUCEL HI520 POM+Rubber, High Impact Feature: Injection Molding, POM+Rubber, High ImpactApplication: GearsCAS No. 66455-31-0 and 155123-66-3Information provided by LG Chemical |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | 60x60x2 mm; ISO 294-4 |
| Gromax BTQ50-DQ00N1 Nylon 6, Impact Modified (Dry) Information provided by Gromax Enterprises Corp. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
| SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing 15% PTFE, 10% Aramid Fiber. Added features of this material include: Wear Resistant. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
| SABIC Innovative Plastics LNP LUBRICOMP RAL23 PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23 is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
| SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing 10% PTFE, 15% Aramid. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.018 cm/cm @Time 86400 sec |
0.017 - 0.018 in/in @Time 24.0 hour |
ASTM D955 |
| SABIC Innovative Plastics LNP LUBRICOMP RAL23S PA 66 (Asia Pacific) LNP LUBRICOMP* RAL23S is a compound based on Nylon 66 resin containing Aramid Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | |
| Solvay Specialty Polymers KetaSpire® KT-880 NL Polyetheretherketone (PEEK) KetaSpire® KT-880 NL is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire® PEEK is produced to the highest industry.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.023 cm/cm @Thickness 3.20 mm |
0.017 - 0.023 in/in @Thickness 0.126 in |
SABIC Method |
| SABIC Innovative Plastics Valox® 315 PBT (Asia Pacific) General purpose polyester. Fully imported product from USA |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 3.17 mm |
0.017 in/in @Thickness 0.125 in |
ASTM D955 |
| Techmer ES HiFill® PA12 Availability: North AmericaForms: PelletsFeatures: Low ViscosityTPCI# 8807105Information provided by TP Composites, Inc. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | 24 hours + 30 min at 93°C |
| Teknor Apex TEKRON® 4300LM-P86-1 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.019 cm/cm | 0.017 - 0.019 in/in | ISO DIS 294-4 |
| Wellman Wellamid® NY1733-GY1 Lubricated, Nucleated, Unfilled Nylon 6 Description: Lubricated, Nucleated, Unfilled Nylon 6Information provided by Wellman. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
| DuPont Performance Polymers Crastin® 6131 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Crastin 6131 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 2577 |
| DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 4.00 mm |
0.017 in/in @Thickness 0.157 in |
E2P method |
| Eurostar Staramide P1000J5 PA6, Impact Modified, Injection Molded Staramide P1000J5 is a Low Temperature Impact Modified, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Eurotec |
| Eurotec® Tecodur® PB70 NL IL PBT, impact modified, natural Information provided by Eurotec® |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
| Clariant Renol BR2029 Nylon 66, General Purpose, Black Data provided by Clariant Masterbatches |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ISO 294-4 |
| Barlog Plastics KEBAFLEX S 70 A.01 TPE-S, Shore A70, translucent TPE-SInformation provided by BARLOG plastics GmbH. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm @Thickness 2.00 mm |
0.017 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
| DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | 60x60x2mm; ISO 294 |
| BASF Ultradur B 6550 PBT Ultradur B 6550 is a high viscosity PBT extrusion grade.Applications; Used for loose buffer tubes for optical fibers, semi-finished products fro machining, profiles and pipes. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | Sheet |
| BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF |
|||
| Linear Mold Shrinkage, Flow | 0.017 - 0.020 cm/cm | 0.017 - 0.020 in/in | |
| LATI Later 4 PBT Polybutylene Terephthalate (PBT). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A. |
|||
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | SABIC Method |
| SABIC Innovative Plastics LNP Thermotuf P1000J5 PA 6 (Europe-Africa-Middle East) LNP* THERMOTUF* P1000J5 is a compound based on PA 6 resin containing Impact Modifier.
Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||