Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.32 g/cc | 0.0477 lb/in³ | ISO 1183 |
Moisture Absorption | 2.00 % @Temperature 23.0 °C |
2.00 % @Temperature 73.4 °F |
50% RH; ISO 62 |
Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | Eurotec |
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | Eurotec |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 170 MPa | 24700 psi | ISO 527 |
Elongation at Break | 3.0 % | 3.0 % | ISO 527 |
Tensile Modulus | 8.50 GPa | 1230 ksi | ISO 527 |
Izod Impact, Notched (ISO) | 8.00 kJ/m² @Temperature -30.0 °C |
3.81 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
10.0 kJ/m² @Temperature 23.0 °C |
4.76 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A | |
Izod Impact, Unnotched (ISO) | 60.0 kJ/m² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1U |
65.0 kJ/m² @Temperature 23.0 °C |
30.9 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1U |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 262 °C | 504 °F | [10 K/min], ISO 11357 |
Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F | ISO 75 |
Deflection Temperature at 1.8 MPa (264 psi) | 250 °C | 482 °F | ISO 75 |
Vicat Softening Point | 255 °C @Load 5.10 kg |
491 °F @Load 11.2 lb |
ISO 306 |
Flammability, UL94 | HB @Thickness 0.750 mm |
HB @Thickness 0.0295 in |
|
HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F | Throat |
Mold Temperature | 70.0 - 110 °C | 158 - 230 °F | |
Drying Temperature | 80.0 °C | 176 °F | |
Dry Time | 2.00 - 4.00 hour | 2.00 - 4.00 hour | |
Moisture Content | <= 0.20 % | <= 0.20 % | ISO 960 |
Hold Pressure | 50.0 - 100 MPa | 7250 - 14500 psi |
Descriptive Properties | Value | Comments |
---|---|---|
Back Pressure | Low | |
Injection Speed | Fast |