| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 40% Glass Fiber Filled |
| Manufacturer | DuPont Performance Polymers |
| Trade Name | Zytel® PLS |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6
(Unverified Data**).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.40 g/cc | 0.0506 lb/in³ | DAM; ISO 1183 |
| Moisture Absorption | 2.00 % <br>@Thickness 2.00 mm |
2.00 % <br>@Thickness 0.0787 in |
DAM; Sim. to ISO 62 |
| Linear Mold Shrinkage, Flow | 0.0020 cm/cm | 0.0020 in/in | DAM; ISO 294-4 2577 |
| Linear Mold Shrinkage, Transverse | 0.0070 cm/cm | 0.0070 in/in | DAM; ISO 294-4 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 120 MPa | 17400 psi | 50%RH; ISO 527-1/-2 |
| 197 MPa | 28600 psi | DAM; ISO 527-1/-2 | |
| Elongation at Break | 3.5 % | 3.5 % | DAM; ISO 527-1/-2 |
| 7.0 % | 7.0 % | 50%RH; ISO 527-1/-2 | |
| Tensile Modulus | 6.50 GPa | 943 ksi | 50%RH; ISO 527-1/-2 |
| 11.5 GPa | 1670 ksi | DAM; ISO 527-1/-2 | |
| Flexural Strength | 309 MPa | 44800 psi | DAM; ISO 178 |
| Flexural Modulus | 10.1 GPa | 1460 ksi | DAM; ISO 178 |
| Charpy Impact Unnotched | 9.30 J/cm² | 44.3 ft-lb/in² | 50%RH; ISO 179/1eU |
| 9.60 J/cm² | 45.7 ft-lb/in² | DAM; ISO 179/1eU | |
| 8.10 J/cm² <br>@Temperature -30.0 °C |
38.5 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eU | |
| 8.30 J/cm² <br>@Temperature -30.0 °C |
39.5 ft-lb/in² <br>@Temperature -22.0 °F |
50%RH; ISO 179/1eU | |
| Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | DAM; ISO 179/1eA |
| 1.30 J/cm² <br>@Temperature -30.0 °C |
6.19 ft-lb/in² <br>@Temperature -22.0 °F |
DAM; ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 3.00 µm/m-°C | 1.67 µin/in-°F | DAM; ISO 11359-1/-2 |
| CTE, linear, Transverse to Flow | 10.0 µm/m-°C | 5.56 µin/in-°F | DAM; ISO 11359-1/-2 |
| Melting Point | 224 °C | 435 °F | DAM; 10°C/min; ISO 11357-1/-3 |
| Deflection Temperature at 0.46 MPa (66 psi) | 220 °C | 428 °F | DAM; ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 212 °C | 414 °F | DAM; ISO 75-1/-2 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 7.10e+13 ohm-cm | 7.10e+13 ohm-cm | 50%RH; IEC 60093 |
| >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm | DAM; IEC 60093 | |
| Surface Resistance | 6.10e+13 ohm | 6.10e+13 ohm | 50%RH; IEC 60093 |
| Comparative Tracking Index | 550 V | 550 V | DAM; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Part Marking Code | >PA6-GF35< | ISO 11469 |
| Processing | Injection Moulding | |
| Regional Availability | Asia Pacific | |
| Europe | ||
| Global | ||
| Near East/Africa | ||
| North America | ||
| South and Central America | ||
| Resin Identification | PA6-GF35 | |
| Special Characteristics | Heat stabilised or stable to heat |