Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Versaflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Versaflex™ OM 1060X-9 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Versaflex™ OM 1060X-9 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Excellent Bond to PC, ABS, PC/ABS - Good Surface Aesthetics - Rubbery Feel - Soft TouchPurge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Versaflex™ OM 1060X-9 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versaflex™ OM 1060X-9 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 5 - 8 minutes or longer. Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 350 to 800 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 3 to 10 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.928 g/cc
0.928 g/cc
ASTM D792
Viscosity 11700 cP

@Shear Rate 11200 1/s,
Temperature 200 °C
11700 cP

@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.0080 - 0.013 cm/cm
0.0080 - 0.013 in/in
ASTM D955
Melt Flow 19 g/10 min

@Load 2.16 kg,
Temperature 190 °C
19 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
29 g/10 min

@Load 5.00 kg,
Temperature 200 °C
29 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 sec; ASTM D2240
Tensile Strength at Break 3.79 MPa

@Temperature 23.0 °C
550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 2.14 MPa

@Strain 100 %,
Temperature 23.0 °C
310 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
3.24 MPa

@Strain 300 %,
Temperature 23.0 °C
470 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 510 %

@Temperature 23.0 °C
510 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 26.3 kN/m
150 pli
ASTM D624
Compression Set 29 %

@Temperature 23.0 °C,
Time 79200 sec
29 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94
Processing Properties Metric English Comments
Rear Barrel Temperature 166 - 188 °C
331 - 370 °F
Middle Barrel Temperature 182 - 193 °C
360 - 379 °F
Front Barrel Temperature 193 - 227 °C
379 - 441 °F
Nozzle Temperature 199 - 232 °C
390 - 450 °F
Melt Temperature 193 - 227 °C
379 - 441 °F
Mold Temperature 21.1 - 37.8 °C
70.0 - 100 °F
Back Pressure 0.000 - 0.862 MPa
0.000 - 125 psi
Screw Speed 75 - 125 rpm
75 - 125 rpm
Descriptive Properties Value Comments
Agency Ratings UL 94 .QMFZ2.E76261
Appearance Black
Features Good Moldability
Good Processability
Good Processing Stability
Good Surface Finish
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Suggested Max Regrind 20%
Uses Consumer Applications
Electrical/Electronic Applications
Flexible Grips
Overmolding
Power/Other Tools
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved