Polymer Property : Tensile Modulus = 11.5 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527-1/-2
DSM Akulon® S223-G8U (Dry) 43% Glass Reinforced Nylon 66 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 11.5 GPa
1670 ksi
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo..
Tensile Modulus 11.5 GPa
1670 ksi
d.a.m.; ISO 527-1, -2; 1 mm/min
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527-1,-2
Lanxess Durethan® AKV 35 LT H3.0 000000 Nylon 66, 35% Glass Fiber
PA 66, 35% glass fiberInformation provided by LANXESS.
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527-1/-2
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in..
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM 2400F PEI (Europe-Africa-Middle East)
40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. US FDA and European Food Contact approved. Effective June, 2007 this grade will no longer be..
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific)
33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE.
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics ULTEM HU2410 PEI
40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP..
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific)
Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT..
Tensile Modulus 11.5 GPa
1670 ksi
dry; ISO 527-1/-2
DSM Akulon® XG-FKGS6 PA6-GF30 FR
30% Glass Reinforced, Flame Retardant, Halogen free
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50
Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w..
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® LV-5H PA12-GF50
Product description: Grilamid LV-5H is a 50% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30
Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya..
Tensile Modulus 11.5 GPa
1670 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30
Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya..
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527-1/-2
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont ..
Tensile Modulus 11.5 GPa
1670 ksi
50%RH; ISO 527-1/-2
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 51G35NOX BK420 Polyphthalamide (PPA)
Zytel® HTN51G35NOX BK083 is a 35% glass reinforced high performance polyamide resin developed for Selective Catalytic Reduction applications that require exposure to water/urea solution. It is also..
Tensile Modulus 11.5 GPa
1670 ksi
DAM; ISO 527-1/-2
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation ..
Tensile Modulus 11.5 GPa
1670 ksi
1 mm/min; ISO 527
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded
Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T..
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® BG-50 H PA6-GF50
Product description: Grilon BG-50 H is a high heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 H has the following important properties: High stiffnessHigh heat resist..
Tensile Modulus 11.5 GPa
1670 ksi
conditioned; ISO 527-1/-2
EMS-Grivory Grivory® BG-50 S PA6-GF50
Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin..
Tensile Modulus 11.5 GPa
1670 ksi
dry; ISO 527-1/-2
EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65
Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and ph..
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade
Information provided by Eurotec®
Tensile Modulus 11.5 GPa

@Treatment Temp. 70.0 °C,
Time 522000 sec
1670 ksi

@Treatment Temp. 158 °F,
Time 145 hour
62% rel. humidity
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
Tensile Modulus 11.5 GPa
1670 ksi
ISO 527-1/-2
DSM Akulon® K-FKGS6 (Dry) 30% Glass Reinforced Nylon 6 (North America)  (discontinued **)
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
ISO 527-2
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength..
Tensile Modulus 11.5 GPa

@Temperature 23.0 °C
1670 ksi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Zytel® HTN 51G35HSLR BK420J Polyphthalamide (PPA)  (Unverified Data**)
Zytel® HTN51G35HSLR BK420J is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin with improved hydrolysis resistance and surface appearance. It is also a PPA resin..