Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 220 °C Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 220 °C

@Thickness 3.20 mm
428 °F

@Thickness 0.126 in
unannealed; ASTM D648
Ovation Polymers UTTAP QU HT530 GF Nylon, 30% Glass Reinforced
Glass reinforced (30 %) - High Temperature Polyamide Alloy, excellent chemical and electrical resistance, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Nilit FRIANYL B63 KF30 Nylon 6 for injection molding, 30% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Nilit FRIANYL B63 KF50 Nylon 6 for injection molding, 50% short glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
DIN 53461; ASTM D648
Kolon SPESIN® KP213G45 Flame Retardant PBT Resin  (discontinued **)
SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
120°C/h; ISO 75/1
Polykemi AB POLYshine PBT D203 GF30 FR PBT, Glass Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Nilit FRIANYL B63 H-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced
Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
Nilit FRIANYL B63 HS-GV30 Nylon 6 for injection molding, 30% glass fiber reinforced
Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
DSM Akulon® Ultraflow™ K-FHG7 Nylon 6-35% Glass Reinforced (European Grade) (Dry)  (discontinued **)
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier ..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Kolon SPESIN® KP213G20WBL Glass Fiber Reinforced & Weather Resistant PBT Compound Resin
G/F 20% reinforced, weather resistanceApplications: Parts of electric lightInformation provided by API-Kolon.
Deflection Temperature at 0.46 MPa (66 psi) 220 °C

@Thickness 6.40 mm
428 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical Lupox® GP2400G PBT+GF40%
Description: Injection Molding, PBT+GF40%, HCFC ResistantApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 30965-26-5Information provided by LG Chemical
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced
High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
SABIC Innovative Plastics LNP Thermocomp PF006 PA 6 (Europe-Africa-Middle East)
30% glass fibre reinforced Polyamide 6 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
0.25 inch; ASTM D648
PlastxWorld CEVIAN® B5726 30% GF PBT/ABS Alloy
Glass fiber reinforced, heat resistant and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Toyobo Vylopet® EMC615 PET/PBT Blend
Key Feature: Flame retardant V-0 UL 94 classApplications: electrical and electronic componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
dry; ISO 75-1/-2
DSM Novamid® 1015GH35 BK37 PA6-GF35
35% Glass Reinforced, Heat Stabilized, Injection Molding
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
dry; ISO 75-1/-2
DSM Novamid® 1017GH33 BK701 PA6-GF33
33% Glass Reinforced, Heat Stabilized, Injection Molding
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
Edgew 120x10x4, sp=100 mm; ISO 75/Be
Eurostar Staramide PF006 PA6, 30% Glass Fiber Filled, Injection Molded
Staramide PF06 is an 30% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
Barlog Plastics KEBATER BF250 PBT, 50% glass fiber reinforced, food grade
PBT-GF50Information provided by BARLOG plastics GmbH.
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75
BASF Ultradur B 4040 G10 High Speed BK15029 50% Glass Filled PBT/PET
Ultradur B 4040 G10 High Speed BK15029 is a high flow, fast cycling with low warpage, 50% glass filled, injection molding PBT for industrial parts, rigid tough and dimensional stable applications.
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-2
BASF Ultradur B 4300 G4 20% Glass Filled PBT
Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
BASF Ultramid® B3EG5 25% Glass Filled PA6 (Dry)
Description: 25% glass-fiber reinforced injection-molding grade for industrial articles and electrical insulating partsInformation provided by BASF
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM D648
Cheng Yu Plastic FR200N Flame Retardant Nylon 66
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
BASF Ultramid® A4H PA66 (Dry)
Description: Highly heat aging resistant, medium-viscosity injection-molding grade for highly stressed parts such as bearing cages, gearwheels, spool bodies and chain drive tensioners.Information pr..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO 75-1/-2
DSM Arnite® TV4 260 S PBT-30% Glass Reinforced (European and Asian Grade)
Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame ..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ISO data
BASF Capron® GR30 HS 30% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron GR30 HS is a heat stabilized 30% glass reinforced polyamide 6 injection molding compound possessing a balance of engineering properties combined with excellent processability and surface aest..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C

@Thickness 3.20 mm
428 °F

@Thickness 0.126 in
unannealed; ASTM D648
SABIC Innovative Plastics LNP THERMOCOMP 9X11427
LNP* THERMOCOMP* 9X11427 is a compound based on Miscellanbeous resin containing 40% specialty glass filled TP alloy. Added features of this grade include: Ultra-Stiff Toughness, Improved Impact, G..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
LATI Latilub 75/4-05T G/30-V0 PBT, 30% Glass Fiber Reinforced, PTFE Filled, Flame Retardant
Self-lubricating product based on Polybutylene Terephthalate (PBT). PTFE. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Afri..
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
428 °F
ASTM Test
BASF Ultramid® B3WG6 BK00564 BGVW 30% Glass Filled PA6 (Dry)
Ultramid B3WG6 BK00564 BGVW is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade.
Copyright © lookpolymers.com All Rights Reserved