| Category | Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade |
| Manufacturer | Clariant |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Clariant Renol 6253 Nylon 6, High Impact.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.10 g/cc | 1.10 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.017 cm/cm | 0.017 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 62.1 MPa | 9000 psi | ASTM D638 |
| Elongation at Yield | 100 % | 100 % | ASTM D638 |
| Flexural Yield Strength | 89.6 MPa | 13000 psi | ASTM D790 |
| Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
| Izod Impact, Notched | 1.60 J/cm <br>@Temperature 22.8 °C |
3.00 ft-lb/in <br>@Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 171 °C | 340 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 60.0 °C | 140 °F | ASTM D648 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 254 - 271 °C | 490 - 520 °F | |
| Mold Temperature | 51.7 - 79.4 °C | 125 - 175 °F | |
| Dry Time | 2 - 4 hour <br>@Temperature 79.4 °C |
2 - 4 hour <br>@Temperature 175 °F |
to ensure moisture content is less than 0.2% |
| Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
| 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial | |
| Back Pressure | 0.345 - 1.72 MPa | 50.0 - 250 psi | |
| Shot Size | 30 - 80 % | 30 - 80 % | |
| Screw Speed | 20 - 100 rpm | 20 - 100 rpm |