Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® S190A Thermoplastic Polyurethane Type: Estane® S190A is a Shore 92A, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: AsiaInformation Provided by The.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T365A Thermoplastic Polyurethane Type: Estane® T365A is a Shore 70A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Cor.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T460A Thermoplastic Polyurethane Type: Estane® T460A is a Shore 66A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T470A Thermoplastic Polyurethane Type: Estane® T470A is a Shore 77A, polyester grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant 612-01 HSL Black Nylon 612, Heat Stabilized Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 6601FR Nylon 66, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol ABS3460 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA111G60 Nylon 66, 60% Glass Fiber Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113C Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113G13 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113G13X050 Nylon 66, 13% Glass Fiber, Heat Stabilized, Lubricated, Improved Ductility Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0009HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0011HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0013WT-192 Polycarbonate, Flame Retardant, UV Stabilized, High Opacity Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PP1100G40 Polypropylene Homopolymer, 40% Glass Fiber, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PP1112AS10 Polypropylene, Static Dissipative Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSP0006HW Polypropylene Homopolymer, Heavy Weight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol R60G33HSL Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated, Economy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA111G30IF Nylon 66, 30% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T865A Thermoplastic Polyurethane Type: Estane® T865A is a Shore 71A, polyester grade, plasticized low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Information Provided by The Lubrizol Corporation |