| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Omni Plastics OmniTuff™ CPP GRC30 Copolymer Polypropylene Glass Reinforced Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| SABIC Innovative Plastics Cycoloy® FXC630ME PC+ABS (Asia Pacific) PC+ABS, ECO-conforming flame retardant with metallic or pearlescent appearance. |
|||
| Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Polymer Resources TP-IM-G7.5 Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact Modified Polybutylene Terephthalate, 7.5% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Polymer Resources NY6-IM1-[color]H Nylon, Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | 73°F; ASTM D256 |
| LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer Description: Pro-faxâ„¢ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Temperature 23.0 °C |
3.00 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
| SABIC Innovative Plastics LNP Lubricomp DP003F PC (Asia Pacific) LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | natural, tints; ASTM D256 |
| SABIC Innovative Plastics ULTEM CRS5311 PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 and 5VA listing. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Techmer ES HiFill FR® PA6 FR IM 004 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Solvay Specialty Polymers Radel® R-7558 Polyphenylsulfone (PPSU) Radel® R-7558 polyphenylsulfone resin is a cost-effective solution for aircraft interior applications. This product complies with the FAA regulation 14CFR Part 25 Appendix F, offering vertical bu.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Techmer ES HiFill® PA6/6 GF40 HS L 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedInformati.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Techmer ES HiFill® PA6/6 GF40 HS L BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | 73°F, 0.125 in.; ASTM D256 |
| Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D 638 |
| Styrolution PS 5801 HIPS Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM Data |
| Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
| Izod Impact, Notched | 1.60 J/cm @Temperature -40.0 °C |
3.00 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
| SABIC Innovative Plastics NORYL PX1390 PPE+PS (Asia Pacific) Automotive applications, primarily. Excellent electrical properties, easy processability, high heat, 295F (146C) DTUL. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Plastics Group Polifil® RP-ABS Acrylonitrile-Butadiene Styrene, Standard Version Polifil® RP- Acrylonitrile-Butadiene Styrene is a styrenic resin with improved toughness and heat resistance versus HIPS grades. ABS exhibits high gloss, low shrinkage, and good dimensional stabili.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Chase Plastics CP Pryme® NN200L (COND, 50% RH) Nylon 66, Internally Lubricated Information provided by Chase Plastics. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Total PSI 945E Polystyrene Polystyrene 945E is a high impact polystyrene designed for applications requiring extra toughness without sacrificing mechanical properties. Excellent falling dart impact combined with the high glos.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | At 73°F; ASTM D256 |
| Plastics Group Polifil® GFRMPPCC-20 20% Glass Reinforced Polypropylene, High Impact Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap.. |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Toyobo Vylopet® EMC630 PET/PBT Blend Key Feature: Flame retardant V-0 UL 94 classApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, go.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 3.17 mm |
3.00 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
| Entec Hypro™ PPC-GF20 Natural Impact Polypropylene, 20% Glass Reinforced Information provided by Entec |
|||
| Izod Impact, Notched | 1.60 J/cm @Temperature 22.8 °C |
3.00 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
| Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized Data provided by Clariant Masterbatches |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | ASTM D256 |
| Asahi Kasei Thermylene® P6-20FG-1734 20% Glass Fiber Reinforced, High Impact Information provided by Asahi Thermofil |
|||
| Izod Impact, Notched | 1.60 J/cm | 3.00 ft-lb/in | reverse notched; ASTM D256 |
| Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
3.00 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
| Premix Thermoplastics PRE-ELEC® ESD 12-000
(discontinued **) PRE-ELEC ESD 12-000 is a static dissipative thermoplastic compound based on polyacetal copolymer. The dissipative property is permanent and built into the polymer chain. The products made out of PRE.. |
|||
| Izod Impact, Notched | 1.60 J/cm @Temperature -30.0 °C |
3.00 ft-lb/in @Temperature -22.0 °F |
PB; ASTM D256 |
| Solvay Engineered Polymers SEQUEL® E3000 HMS TPO
(discontinued **) Description: SEQUEL® E3000HMS thermoplastic olefinic elastomer (TPO) is designed for exterior and interior applications that require stiffness and durability. This extrusion-grade material is spec.. |
|||