| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 g/cc | 0.0376 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.0040 cm/cm | 0.0040 in/in | MD; ASTM D955 |
| Melt Flow | 2.2 g/10 min | 2.2 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 107 | 107 | ASTM D785 |
| Tensile Strength at Break | 33.0 MPa | 4790 psi | ASTM D638 |
| Tensile Strength, Yield | 47.0 MPa | 6820 psi | ASTM D638 |
| Elongation at Break | 25 % | 25 % | ASTM D638 |
| Elongation at Yield | 4.0 % | 4.0 % | ASTM D638 |
| Tensile Modulus | 2.099 GPa | 304.5 ksi | ASTM D638 |
| Flexural Strength | 77.01 MPa | 11170 psi | ASTM D790 |
| Flexural Modulus | 2.80 GPa | 406 ksi | ASTM D790 |
| Izod Impact, Notched | 2.24 J/cm | 4.20 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 90.0 °C | 194 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 77.2 °C | 171 °F |