Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® S392A Thermoplastic Polyurethane Type: Estane® S392A is a Shore 93A, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding, Extrusion, Blow .. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | |
Lubrizol Estane® T370A Thermoplastic Polyurethane Type: Estane® T370A is a Shore 74A, polyether grade, plasticizer-free, with low hardness thermoplastic polyurethane (TPU).Uses: Injection Molding, Extrusion.Availability: AsiaInformation Provided b.. |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA131G2GN-91 Green Nylon 66, Highly Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant PA621G30 Nylon 612, 30% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 60G13HSP Black Nylon 6, 13% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 612G10-L Nylon 612, 10% Glass Fiber Reinforced, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol 66G33HSL Nylon 66, 33% Glass Fiber Reinforced, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR7039 Nylon 6 Alloy, bondable to TPU Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol BR7140 Polycarbonate/ABS Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA111G20CF10BK Nylon 66, 20% Glass and 10% Carbon Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA111G50IF Nylon 66, 50% Glass Fiber, Improved Flow Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA113G33HR Nylon 66, 33% Glass Fiber, Heat Stabilized, Hydrolysis Resistant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0004 Nylon 6 Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1700 Polybutylene Terephthalate, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PBTG30-L Polybutylene Terephthalate, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0006GY-371 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0010 Polycarbonate Alloy, Glass Fiber and Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PCSP0011 Polycarbonate Alloy, Glass Fiber and Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol POMSP0001 Acetal Copolymer, Aramid Fiber, PTFE Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSP0005 Polypropylene Homopolymer, Glass Fiber and Mica Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSS0007 Polyphenylene Sulfide, Glass Fiber and Mineral Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 8.27 - 13.8 MPa | 1200 - 2000 psi | Initial |
Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled Data provided by Clariant Masterbatches |