Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.28 GPa | 330 ksi | Tangent; ASTM D790 |
RheTech Products HP532-01 20% Talc Reinforced High Performance Polypropylene, Non-UV Stabilized, Black Applications: Close out panelSpeaker grilleInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources ABS-GP1-[color]-3 ABS, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC/ABS-GP1-[color]-UV General Purpose PC/ABS Alloy, UV-stabilized PC/ABS Alloy, General Purpose, UV-stabilized Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provide.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC-FD4-[color]-1 Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow with Mold Release, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S459HTP ABS + Polycarbonate Alloy Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Polymer Resources PC-FD4 Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma Resistant Polycarbonate, FDA-compliant Feedstocks, Easy Flow, Gamma ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
LTL Color Compounds ColorRxâ„¢ PC-1002AF Food Grade Polycarbonate A biocompatible, 10 melt grade of Polycarbonate for healthcare applications, containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Spartech Royalite R71/920 PC/ABS Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES HiFill® POM 0212B Acetal Availability: North AmericaForms: PelletsFeatures: Copolymer and High Specific GravityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS LE BK Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC300RHF Polycarbonate, Recycled Content Features: Good flowHigh rigidityGood toughnessHigh strengthLow viscosityGood mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC300RUV Polycarbonate (Utility Grade), UV Stabilizer, Mold Release Information provided by Chase Plastics. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | Tangent, chs 0.05 in/min; ASTM D790 |
Diamond Polymers ABS 3002MC Description: Plating GradeInformation provided by Diamond Polymers, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Clariant ABS4500 ABS, High Impact Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Clariant Renol BR7008 Polycarbonate/Polyester Alloy Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Clariant Renol PCSP0006 Polycarbonate, Laser Markable Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D-790 |
Axiall UV-6676 Rigid PVC, Molding Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as .. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Amco Amalloy® B9336 Polymer Alloy Amco Amalloy B9336 is a clear performance copolymer with exceptional clarity and toughness.Stiff, with good tensile and flexural strength.Information provided by Amco Plastic Materials. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Techmer ES Plastiblend® ABS 8008 Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 2.28 GPa | 330 ksi | ASTM D790 |
Amco Amalloy® B9941 Polymer Alloy Amco Amalloy B9941 is a clear performance copolymer with exceptional clarity and toughness.Good flexural and tensile strength.Information provided by Amco Plastic Materials. |