Polymer Property : Specific Gravity = 1.10 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Liquid State
Palm Labs Adhesives Turbo Fuse Series 130PR PLASTIC & RUBBER (100 Viscosity) Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130PR PLASTIC & RUBBER’S advanced formula is designed to polymerize instantly by absorbing surface moisture. Th..
Specific Gravity 1.10 g/cc
1.10 g/cc
Palm Labs Adhesives TURBO SEAL SERIES 50 PURPLE FLEXIBLE GASKET SEALANT
TURBO SEAL SERIES 50 is an anaerobic gasket sealant, which develops medium strength in a short time. The compound cures in the absence of air between close fitting surfaces and will flex with minor ..
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Permabond HH131 High Temperature Threadlocker
Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for ..
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Permabond HM128 Anaerobic Threadlocker
Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked..
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Permabond LH150 Anaerobic Threadsealant
Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up ..
Specific Gravity 1.10 g/cc
1.10 g/cc
Palm Labs Adhesives TURBO-LOCK SERIES 17-GP Anaerobic Thread Locking Compound
BEARING AND SHAFT - SERIES 17-GP is a fast curing, GREEN, high strength, general purpose, press fit, anaerobic retaining compound for bonding, sealing and retaining of cylindrical parts. It is highl..
Specific Gravity 1.10 g/cc
1.10 g/cc
Resinlab® CYNERGY CA6501 Adhesive
Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa..
Specific Gravity 1.10 g/cc
1.10 g/cc
Momentive Performance Materials Siloprenâ„¢ LSR 2730 Liquid Silicone Rubber - Self-Bonding
This LSR elastomer is a self-bonding, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatur..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Samsung Cheil Industries Starex® EG-7000 ABS/PET, Unreinforced
Information provided by Samsung Cheil Industries.
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Samsung Cheil Industries Starex® TF-0930 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Teknor Apex Monprene® MP-2123 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
SABIC Innovative Plastics NORYL N190HF PPE+HIPS (Asia Pacific)
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Samyang Trimma® SD6320 PMMA, Translucent
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Applications: Laptop, Monitor Front Cover - for high flow, high gloss and high hardnessInformat..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1697HU High Flow Fortified Polypropylene
DescriptionPolyfort® FPP 1697HU is a high flow fortified polypropylene with high temperature dimensioned stability. It is stabilized for UV exposure and available in matched automotive color.Infor..
Specific Gravity 1.10 g/cc
1.10 g/cc
Zeon Chemicals HyTemp® 4051CG AR Polyacrylate Elastomer
HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Cement grade version of Hy..
Specific Gravity 1.10 g/cc
1.10 g/cc
Zeon Chemicals HyTemp® 4451CG AR Polyacrylate Elastomer
HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Particulate version of HyT..
Specific Gravity 1.10 g/cc
1.10 g/cc
Mixed
Tra-Con Tra-Bond FDA2YL02 Food and Drug Application Epoxy Adhesive
TRA-BOND FDA-2 YL02 is a medium viscosity epoxy resin system specifically developed for adhesive and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Denka TP-803 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Clariant 6604-HSL Nylon 66, Impact Modified, Heat Stabilized
Data provided by Clariant Masterbatches
Specific Gravity 1.10 g/cc
1.10 g/cc
BCC Products BC 5008-2 General Purpose Epoxy System
BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A..
Specific Gravity 1.10 g/cc
1.10 g/cc
BCC Products BC 8160 Urethane Casting
BC8160 is a low viscosity two-component urethane casting compound that is specifically formulated for its flexural and impact strength. It is recommended for use for the production casting of highly..
Specific Gravity 1.10 g/cc
1.10 g/cc
Uncured
Permabond 910FS Cyanoacrylate, Methyl grade
PERMABOND® 910FS is the original 100%-methyl cyanoacrylate adhesive. It is a single part, low viscosity liquid that will cure rapidly at room temperature when pressed into a thin film between parts..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
E-Polymers EFLEX® S1040 General
S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas..
Specific Gravity 1.10 g/cc
1.10 g/cc
Part B
Resinlab® UR3010 Black Polyurethane Potting System
Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific)
Cycoloy Medium Heat Plating Grade for Automotive
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
EG65D Polyurethane-based Biomedical Elastomer