Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 254 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 254 - 266 °C
489 - 511 °F
ASTM D789
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 254 - 266 °C
489 - 511 °F
ASTM D789
Niche Polymer PA66GF50BK Nylon 66, 50% Glass Fiber Filled
Information provided by Niche Polymer
Melt Temperature 254 - 271 °C
489 - 520 °F
ASTM D789
Niche Polymer PA66GM38BK Nylon 66, 38% Glass/Mineral Fiber Filled
Information provided by Niche Polymer
Melt Temperature 254 - 266 °C
489 - 511 °F
ASTM D789
Niche Polymer PA66GM40N Nylon 66, 40% Mineral Fiber Filled
Information provided by Niche Polymer
Melt Temperature 254 - 277 °C
490 - 530 °F
Polymer Resources TP-M30 Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced Warpage
Polybutylene Terephthalate, 30% Mineral Reinforced, Reduced WarpageProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Melt Temperature 254 - 277 °C
490 - 530 °F
Ravago Manufacturing Americas Hylon® N2015L Nylon 6 (Cond)
Information provided by Ravago.
Melt Temperature 254 - 277 °C
490 - 530 °F
Ravago Manufacturing Americas Hylon® N2017THL Nylon 6 (DAM)
Information provided by Ravago.
Melt Temperature 254 - 338 °C
490 - 640 °F
Average value: 296 °C Grade Count:7
Overview of materials for Polycarbonate, Foam Grade, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Foam Grade, Glass Filled". Each property range of values reported is minimum and maximum ..
Melt Temperature 254 - 282 °C
490 - 540 °F
Molding
PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated  (discontinued **)
Description/Features:Glass Fiber ReinforcedPTFE LubricatedUL 94 HB (HEM TEST)Information provided by PolyOne Corporation.
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegis™ H85ZP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H85ZP is a medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well as EU..
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegis™ H205QP Nylon 6 Extrusion Grade Homopolymer Film  (discontinued **)
Description: Aegis H205QP is a lubricated high viscosity, N6 film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements of 21 CFR 177.1500. It possesses the combination..
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegisâ„¢ H100MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H100MP is a lubricated and nucleated medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 ..
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegisâ„¢ H135QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H135QP is a lubricated high viscosity, N6, film extrusion grade homopolymer for cast or blown film. It conforms to FDA requirements including, 21 CFR 177.1500 as well as EU Direct..
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegisâ„¢ H155MP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155MP is a lubricated and nucleated high viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. It conforms to Food and Drug Administration requirements of 21 CFR..
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegisâ„¢ H155ZP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H155ZP is a high viscosity, nylon 6 film extrusion grade homopolymer for cast or blown film. It conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 as well a..
Melt Temperature 254 - 260 °C
489 - 500 °F
Tubular (Blown) Film
Honeywell Aegisâ„¢ H85QP Nylon 6 Extrusion Grade Homopolymer Film
Description: Aegis H85QP is a lubricated, medium viscosity, nylon 6 extrusion grade homopolymer for cast or blown film. If conforms to Food and Drugs Administration requirements of 21 CFR 177.1500 a..
Melt Temperature 254 - 277 °C
490 - 530 °F
LTL Color Compounds ColorFast® FRPBT150 PBT, 13% Glass-Filled, Flame Retarded
13% glass-filled V-0 rated PBTAll information provided by LTL Color Compounders, Inc.
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant 6004G8-HSL BK UV Black Nylon 6, 8% Glass Fiber Reinforced
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant PA213M40BK Nylon 6, 40% Mineral Reinforced, Heat Stabilized, Black
Data provided by Clariant Masterbatches
Melt Temperature 254 - 271 °C
490 - 520 °F
Clariant Renol 6253-L UV Nylon 6, High Impact, Lubricated, UV Stabilized
Data provided by Clariant Masterbatches
Melt Temperature 254 - 282 °C
490 - 540 °F
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced
Data provided by Clariant Masterbatches
Melt Temperature 254 °C
489 °F
Chem Polymer Chemlon 217 GI Nylon 6, 17% Glass Fiber Reinforced
A 17% glass fiber reinforced, impact modified nylon 6 offering a combination of creep resistance, stiffness and toughness over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Po..
Melt Temperature 254 °C
489 °F
Chem Polymer Chemlon 225 G Nylon 6, 25% Glass Fiber Reinforced
A 25% glass fiber reinforced nylon 6 offering a balance of properties between the 20% (Chemlon 220 G) and 30% (Chemlon 233 G) product offerings. This product offers further improvements in tensile ..
Melt Temperature 254 °C
489 °F
Chem Polymer Chemlon 225-15 MG Nylon 6, 25% Mineral/15% Glass Fiber Reinforced
A 25% mineral reinforced, 15% glass fiber reinforced nylon 6 offering excellent rigidity, dimensional stability and warpage control in large area parts.Data provided by the manufacturer, Chem Polyme..
Melt Temperature 254 °C
489 °F
Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced
A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 254 °C
489 °F
Chem Polymer Durlex 700 PBT, General Purpose
A lubricated, general purpose PBT.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 254 °C
489 °F
Chem Polymer Durlex 709 IH PBT, Impact Modified
A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 254 °C
489 °F
Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced
A lubricated, 15% glass reinforced PBT offering a balance of rigidity, dimensional stability and toughness.Data provided by the manufacturer, Chem Polymer.
Melt Temperature 254 °C
489 °F
Chem Polymer Durlex 730 GVH PBT, 30% Glass Fiber Reinforced
A glass fiber reinforced, flame retardant PBT exhibiting excellent strength, dimensional stability and elevated temperature performance. The material has a V0 flammability rating according to UL94 ..
Copyright © lookpolymers.com All Rights Reserved